Teijin Chemical, founded in 1918, has been at the forefront of promoting sustainability through robust research and development initiatives aimed at reducing environmental impact. Headquartered in Osaka, Japan, Teijin Chemical core focus: High-performance plastics, polycarbonate resins, and advanced engineering compounds.

At Suke Plastics, we mainly supply:

  • Teijin PEN TN-8065S
teijin chemicals 25kg package

Teijin available for bulk purchase

TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Application
PENTN-8065STEIJIN CHEMICALS General injection molding grade, low oxygen permeability, good barrier performance, 80 MPa tensile strength, No Break unnotched Charpy impactBarrier packaging parts; precision injection molded parts; electronic housings; heat-resistant functional parts; medical/healthcare packaging components