Yuntianhua Group
- Home /
- Yuntianhua Group Company
Plastic Resin Brands We Supply
Yuntianhua
Yuntianhua Group Co., Ltd. is a large comprehensive industrial group in China, with core businesses covering fertilizers, glass fiber and composite materials, and new chemical materials. The group is recognized as one of the leading manufacturers of phosphate fertilizer, nitrogen fertilizer, glass fiber, and acetal copolymer materials.
In the field of engineering plastics, Yuntianhua has built strong capabilities in polyoxymethylene resin, especially acetal copolymer / POM copolymer production, research, grade development, and technical service.
At Suke Plastics, we provide YUNCON® POM resin pellets to customers who need reliable acetal copolymer materials for injection molding, extrusion, modification, and engineering applications.
POM available for bulk purchase
| Type | Grade No. | Manufacturer | Brand | Grade/Features | Use/Applications |
|---|---|---|---|---|---|
| POM | M25 | YUNTIANHUA | Yuntianhua® | High-impact, high-elongation grade, with increased molecular weight | Extruded rods, Extruded sheets, roller conveyor parts |
| POM | M270 | YUNTIANHUA | Yuntianhua® | High-flow grad, with minimized mold deposit | Lighters, aerosol bottles, fasteners |
| POM | SF-5 | YUNTIANHUA | Yuntianhua® | filled with ca.5% PTFE, Highly improved friction and abrasion coefficient than standard grade. | To make the abrasion resistanting objects such as gears, rollers and other silders, especially suit for the environments of without oil or less oil. |
| POM | SF-10 | YUNTIANHUA | Yuntianhua® | filled with ca.10% PTFE, Highly improved friction and abrasion coefficient than standard grade. | To make the abrasion resistanting objects such as gears, rollers and other silders, especially suit for the environments of without oil or less oil. |
| POM | ST-10 | YUNTIANHUA | Yuntianhua® | elastomer-containing, Higher impact resistance and toughness than standard grade M90, fatigue resistance, wear resistance and chemical resistance. | Spoiler Cli, Bumper Clip, Mudguard Clip, Gear, Sleeve, Gasket |
| POM | ST-20 | YUNTIANHUA | Yuntianhua® | elastomer-containing, Higher impact resistance and toughness than standard grade M90, fatigue resistance, wear resistance and chemical resistance. | Spoiler Cli, Bumper Clip, Mudguard Clip, Gear, Sleeve, Gasket |
| POM | GF-10 | YUNTIANHUA | Yuntianhua® | Reinforced with ca.. 10% glass fibers, Improved mechanical properties (stiffness, fatigue resistance, creep resistance etc.) and enhanced HDT up to 150°C | The Cover of Oil Box, The Cover of Radiator, Valve, Gear, Bearing, Cam, Accelerator Pedal, Conveyor Belt, Impeller |
| POM | GF-20 | YUNTIANHUA | Yuntianhua® | Reinforced with ca.. 20% glass fibers, Improved mechanical properties (stiffness, fatigue resistance, creep resistance etc.) and enhanced HDT up to 160°C | The Cover of Oil Box, The Cover of Radiator, Valve, Gear, Bearing, Cam, Accelerator Pedal, Conveyor Belt, Impeller |
| POM | GF-25 | YUNTIANHUA | Yuntianhua® | Reinforced with ca.. 25% glass fibers, Improved mechanical properties (stiffness, fatigue resistance, creep resistance etc.) and enhanced HDT up to 160°C | The Cover of Oil Box, The Cover of Radiator, Valve, Gear, Bearing, Cam, Accelerator Pedal, Conveyor Belt, Impeller |
| POM | EF | YUNTIANHUA | Yuntianhua® | Filled with special lubricant components, Highly improved friction and abrasion coefficient than standard grade. and also with excellent noise resistant, especially suit for the environments of high speed and load. | To make the abrasion resistanting objects such as gears, rollers and other silders, especially suit for the environments of without oil or less oil. |
| POM | FP | YUNTIANHUA | Yuntianhua® | Filled with special lubricant components, Highly improved friction and abrasion coefficient than standard grade. and also with excellent noise resistant, especially suit for the environments of high speed and load. | To make the abrasion resistanting objects such as gears, rollers and other silders, especially suit for the environments of without oil or less oil. |
| POM | MD-1 | YUNTIANHUA | Yuntianhua® | filled with ca.10% PTFE, Highly improved friction and abrasion coefficient than standard grade. | To make the abrasion resistanting objects such as gears, rollers and other silders, especially suit for the environments of without oil or less oil. |
| POM | M90 | YUNTIANHUA | Yuncon® | Standard-flow grade, with minimized mold deposit | Automotive Elecronics, Fittings, Thin-walled Parts, Automotive Exterior Parts, Gears, Valves/Valve Parts, Aumomotive Under the Hood, pining, Wheels, Bearings, Pump Parts |
| POM | GM90 | YUNTIANHUA | Yuncon® | Standard-flow grade, with minimized mold deposit | Automotive Elecronics, Fittings, Thin-walled Parts, Automotive Exterior Parts, Gears, Valves/Valve Parts, Aumomotive Under the Hood, pining, Wheels, Bearings, Pump Parts |
| POM | CM90 | YUNTIANHUA | Yuncon® | Standard-flow grade, with high hardness and high Stiffness | Automotive Elecronics, Fittings, Thin-walled Parts, Automotive Exterior Parts, Gears, Valves/Valve Parts, Aumomotive Under the Hood, pining, Wheels, Bearings, Pump Parts |
| POM | M90-01 | YUNTIANHUA | Yuncon® | Standard-flow grade, with minimized mold deposit | Automotive Elecronics, Fittings, Thin-walled Parts, Automotive Exterior Parts, Gears, Valves/Valve Parts, Aumomotive Under the Hood, pining, Wheels, Bearings, Pump Parts |
| POM | M120 | YUNTIANHUA | Yuncon® | higher flow, with minimized mold deposit | Automotive Elecronics, Fittings, Thin-walled Parts, Automotive Exterior Parts, Gears, Valves/Valve Parts, Aumomotive Under the Hood, pining, Wheels |
| POM | M350 | YUNTIANHUA | Yuncon® | Superhigh-flow grad, with mininized mold deposit | Lighters, aerosol bottles, fasteners |
| POM | M450 | YUNTIANHUA | Yuncon® | Superhigh-flow grad, with mininized mold deposit | Lighters, aerosol bottles, fasteners |
| POM | CN90 | YUNTIANHUA | Yuncon® | Standard-flow grade, with high hardness and high Stiffness | Automotive Elecronics, Fittings, Thin-walled Parts, Automotive Exterior Parts, Gears, Valves/Valve Parts, Aumotive Under the Hood, pining, Wheels, Bearings, Pump Parts |
| POM | N120 | YUNTIANHUA | Yuncon® | with higher flow, with high hardness and high Stiffness | Automotive Elecronics, Fittings, Thin-walled Parts, Automotive Exterior Parts, Gears, Valves/Valve Parts, Aumotive Under the Hood, pining, Wheels |
| POM | N25 | YUNTIANHUA | Yuncon® | High-impact, high-elongation grade, with increased molecular weight | Extruded rods, Extruded sheets, roller conveyor parts |
| POM | N270 | YUNTIANHUA | Yuncon® | High-flow grad, with minimized mold deposit | Lighters, aerosol bottles, fasteners |
| POM | N350 | YUNTIANHUA | Yuncon® | Superhigh-flow grad, with mininized mold deposit | Lighters, aerosol bottles, fasteners |
| POM | N450 | YUNTIANHUA | Yuncon® | Superhigh-flow grad, with mininized mold deposit | Lighters, aerosol bottles, fasteners |
| POM | N90 | YUNTIANHUA | Yuncon® | Standard-flow grade, with minimized mold deposit | Automotive Electronics, Fittings, Thin-walled Parts, Automotive Exterior Parts, Gears, Valves/Valve Parts, Automotive Under the Hood, pining, Wheels, Bearings, Pump Parts |
| POM | N90-01 | YUNTIANHUA | Yuncon® | Standard-flow grade, with minimized mold deposit | Automotive Electronics, Fittings, Thin-walled Parts, Automotive Exterior Parts, Gears, Valves/Valve Parts, Automotive Under the Hood, pining, Wheels, Bearings, Pump Parts |
Main YUNCON® POM Product Series
- General-Purpose POM Grades
- Extrusion Grade POM
- Glass Fiber Reinforced POM
- Toughened POM
- Weather-Resistant and Black POM
- Low Formaldehyde / Special POM Grades
YUNCON® POM Application Areas
- Automotive parts
- Automotive fittings
- Pipe fittings
- Bathroom parts
- Mechanical gears
- Electrical and electronic gears
- Chain plates
- Apparel and textile accessories
- Household chemical packaging parts
- Buckles and fasteners
- Luggage parts
- Oil pump components
- Printer consumables
- Window decoration components
- Toys
- Home appliance components