Chimei WONDERLOY® PC-385

WONDERLOY® PC-385

WONDERLOY® PC-365 General High-heat PC ABS Material

WONDERLOY PC-385 is a top-notch PC/ABS blend. It can take a beating without breaking, even when it’s cold outside. This material is easy to work with, flowing smoothly to fill molds and create complex shapes. It also keeps its cool under heat, staying firm when things get hot. Manufacturers love it because it’s easy to use and helps them make things faster.

  • Application: Automotive interior parts, consumer electronics products, high-end helmets, mobile phone casings, general molding products
  • Character: High heat grade, high impact grade, 1.5mm HB
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Download

Access essential product documentation including technical data sheets, safety information, environmental certifications, and processing guides. All documents are sourced directly from manufacturers and updated regularly for accuracy.

Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=
Chimei WONDERLOY® PC-385 Application

Beatable Strength and Toughness

PC-385 boasts exceptional impact resistance. It stays strong at room temperature and even when it’s freezing, making products more durable and less likely to break.

Flows Like a Dream

This material has excellent flowability. It easily fills molds, allowing manufacturers to create complex shapes and intricate designs with less effort and time.

Keeps Its Cool Under Pressure

PC-385 has a high Vicat softening temperature. This means it maintains its shape and strength even when exposed to high temperatures, perfect for demanding applications.

Chimei WONDERLOY PC-385

WONDERLOY® PC-385 Datasheet

General WONDERLOY® PC-385
Product Description: Ultra high impact
PropertiesISO Test MethodTest ConditionUnitPC-385
Melt Flow Index1133260℃×5KGml/10 min21
Spiral flowCHIMEI260℃,2mm,cm30
V:50%,P:50%
Mass Density118323  ℃g/cm31.15
Tensile Strength52750 mm/min, yieldMPa55
50 mm/min, breakMPa57
Tensile Elongation52750 mm/min%110
Flexural Strength1782 mm/minMPa85
Flexural Modulus1782 mm/minGPa2.3
Izod Impact Strength180/1A23℃, NotchedKJ/m255
-30℃, NotchedKJ/m245
Charpy Impact Strength17923℃, NotchedKJ/m255
-30℃, NotchedKJ/m245
Vicat Softening Temp.30650℃/hr;1KG143
50℃/hr;5KG135
Heat Distortion Temp.75/A1.8MPa, unannealed108
1.8MPa, annealed
Dielectric ConstantIEC 602501MHz3
Volume ResistivityIEC 60093Ohm X m1E+16
Surface ResistivityIEC 60093Ohm1E+16
Coefficient of Linear Thermal Expansion113597.5*10⁻⁵
FlammabilityUL-941.5mm HB
Mold Shrinkage294-4%0.4~0.6
Symbol1043>PC+ABS<
January 12, 2024

WONDERLOY® PC-385 UL Product iQ

WONDERLOY® PC-385 UL Product iQ
File Number: E56070Yellow Card™Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) “WONDERLOY”, furnished as pellets
(+) – Indicate 0~0.5% acid scavengers.
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLHB
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLHB75
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.5 mmPLC 3
3.0 mmPLC 3
High Amp Arc Ignition (HAI)UL 746A
1.5 mmPLC 0
3.0 mmPLC 0
Comparative Tracking Index (CTI)PLC 2UL 746A
Dielectric Strength32   kV/mmASTM D149
High Voltage Arc Tracking Rate (HVTR)PLC 2
Volume Resistivity1.0E+14   ohms·cmASTM D257/IEC 60093
High Voltage, Low Current Arc ResistancePLC 7
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm60   °C
3.0 mm60   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm60   °C
3.0 mm60   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm60   °C
3.0 mm60   °C
PHYSICAL PROPERTIESVALUETEST METHOD
Dimensional Change0.0   %ASTM D1042/ISO 2796
Report Date: 2001-01-12

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top