Polycarbonate + PBT Resin (PC/PBT Resin)
PC PBT resin families
PC/PBT Resin: The Ultimate Engineering Plastic Solution
PC/PBT resin is an advanced polymer blend combining polycarbonate (PC) and polybutylene terephthalate (PBT). This innovative material offers exceptional durability, heat resistance, and chemical resistance, making it ideal for demanding applications across various industries.
As one of the professional PC PBT resin suppliers in China, Suke Plastics specializes in delivering high-quality, reliable, and scalable solutions to meet the needs of modern industries.


PC/PBT Resin Line Card
Key Properties of PC/PBT Resin
Applications of PC/PBT Plastic Alloy

Why Choose Suke Plastics for Your PC/PBT Needs?
Suke Plastics stands at the forefront of PC/PBT resin manufacturing, offering:

PC/PBT vs PC vs PBT
Choosing the Right Material for Your Application
| Property | PC/PBT | PC (Polycarbonate) | PBT (Polybutylene Terephthalate) |
| Composition | Blend of PC and PBT | Polycarbonate | Polybutylene Terephthalate |
| Impact Strength | Excellent | Excellent | Good |
| Chemical Resistance | Good | Fair | Excellent |
| Heat Resistance | Good (120-140°C) | Excellent (125-145°C) | Good (120-130°C) |
| Dimensional Stability | Excellent | Good | Excellent |
| Moisture Absorption | Low | Moderate | Low |
| Electrical Properties | Good | Excellent | Good |
| Processability | Good | Good | Excellent |
| Surface Finish | Good | Excellent | Good |
| Transparency | Opaque to translucent | Transparent | Opaque |
| UV Resistance | Moderate to Good | Poor (unless stabilized) | Good |
| Flame Retardancy | Good (with additives) | Good (with additives) | Good (with additives) |
| Cost | Moderate | Higher | Lower |
| Typical Applications | Automotive parts, electronics, appliances, industrial equipment | Optical applications, safety equipment, medical devices | Electrical components, automotive parts, consumer goods |
| Strength-to-Weight Ratio | High | Very High | Good |
| Wear Resistance | Good | Fair | Excellent |
| Moldability | Good | Good | Excellent |
PC PBT Resin FAQs
Request a Quote Today
Let’s build the future together! Contact us today to discuss your engineering plastics needs or to request a free sample of our premium PC ABS resin. Ready to revolutionize your product line? Your next breakthrough is just a conversation away.