Chimei Polylac® PA-727

Chimei Polylac PA-727 ABS Resin

Polylac® PA-727 Super Impact General ABS Resin

POLYLAC PA-727 is an ABS resin from Chi Mei known for its ultra-high impact resistance and excellent electroplating capabilities. It is ideal for applications in which strength and durability are paramount, such as in the production of pipes, appliances, and large containers. For detailed properties, please refer to the polylac pa 727 datasheet.

  • Application: General molding for decorative accessories, audio equipment panels, tire covers, toiletries, clock casings
  • Character: Ultra-high impact resistance
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Download

Access essential product documentation including technical data sheets, safety information, environmental certifications, and processing guides.
All documents are sourced directly from manufacturers and updated regularly for accuracy.

Chimei Polylac® PA-727 Application

Ultra-High Impact Resistance

This pa 727 abs resin offers superior impact strength with an Izod impact strength of 24 KJ/m2 at 23°C. It ensures that products made with abs polylac pa-727 can withstand substantial mechanical stress without breaking, making it a reliable choice for demanding applications.

Versatile Applications

Chi Mei polylac pa 727 is perfect for a variety of uses, including pipe materials, home appliances, and large containers. Its durability and strength make it suitable for items that need to handle heavier loads and endure wear and tear.

Excellent Thermal Stability

Polylac pa 727 maintains stability under high temperatures, with a Vicat softening temperature of 105°C. This ensures that the resin does not deform or lose its form when subjected to heat. Additionally, its flammability rating of 1.5mm HB under UL-94 standards guarantees that it meets important safety requirements.

Chimei Polylac® PA-727

Polylac® PA-727 Datasheet

Electroplating ABS POLYLAC® PA-727
Product Description: Electroplating
PropertiesISO Test MethodTest ConditionUnitPA-727
Melt Flow Index1133220℃×10KGml/10 min19
Mass Density118323  ℃g/cm31.05
Tensile Strength52750 mm/min, yieldMPa46
50 mm/min, breakMPa34
Tensile Elongation52750 mm/min%50
Flexural Strength1782 mm/minMPa71
Flexural Modulus1782 mm/minGPa2
Izod Impact Strength180/1A23℃, NotchedKJ/m224
-30℃, NotchedKJ/m211
Charpy Impact Strength17923℃, NotchedKJ/m225
-30℃, NotchedKJ/m212
Vicat Softening Temp.30650℃/hr;1KG105
50℃/hr;5KG98
Heat Distortion Temp.75/A1.8MPa, unannealed83
1.8MPa, annealed100
Coefficient of Linear Thermal Expansion113598.8 x 10-5
FlammabilityUL-941.5mm HB
Mold Shrinkage294-4%0.4~0.7
Symbol1043>ABS<
March 11, 2024

Polylac® PA-727 UL Product iQ

POLYLAC® PA-727 UL Product iQ
File Number: E56070Yellow Card™Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLHB
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLHB75
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.5 mmPLC 4
3.0 mmPLC 4
High Amp Arc Ignition (HAI)UL 746A
1.5 mmPLC 0
3.0 mmPLC 0
Comparative Tracking Index (CTI)PLC 1UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 0
High Voltage, Low Current Arc ResistancePLC 7
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm60   °C
3.0 mm60   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm60   °C
3.0 mm60   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm60   °C
3.0 mm60   °C
Report Date: 1983-06-23

Related Polylac® ABS Plastics

No post found!

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top