Chimei ACRYREX® CM-207 PMMA

ACRYREX® PMMA Resin CM-207

ACRYREX® CM-207 PMMA Transparent Grade Medium Strength


Chimei CM-207 PMMA resin is a medium-viscosity Acryrex® material optimized for balanced flowability and strength. Ideal for injection molding, it delivers exceptional clarity, thermal stability (HDT up to 100°C), and durability—perfect for daily necessities, home appliance parts, and precision components requiring glossy finishes and reliable performance.

  • Manufacturer: CHIMEI
  • Character: Medium Strength / Flowability
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 8.5 ml/10 min
  • Tensile Strength: 67 MPa
  • Heat Distortion Temp: 89°C (unannealed), 100°C (annealed)
  • Flammability (1.5 mm): UL 94 HB
  • Mold Shrinkage: 0.2–0.6%

Balanced Flowability & Strength

With a melt flow index of 8.5 ml/10 min, Acryrex CM-207 ensures smooth molding of intricate designs while maintaining tensile strength (67 MPa). Reduces warping in thin-walled appliance housings or kitchenware.

Thermal Stability Under Pressure

Vicat softening at 107°C and heat distortion resistance (89–100°C) make this PMMA resin ideal for heat-exposed parts like hairdryer components or microwaveable containers.

Optical Clarity & Surface Finish

Low mold shrinkage (0.2–0.6%) and UL 94 HB flammability rating ensure glossy, defect-free surfaces for transparent cosmetic jars or LED light covers.

ACRYREX PMMA Resin CM-207

Applications

  • Daily Necessities: Food-grade containers (salad bowls, storage lids), Cosmetic packaging (jars, compacts), Light diffusers for LED lamps.
  • Home Appliance Parts: Transparent blender jugs and coffee maker components, Hairdryer housings and refrigerator door panels, Microwaveable dishware with heat-resistant clarity.
Chimei ACRYREX PMMA Resin CM-207 Application

Acryrex® CM-207 Datasheet

General PMMA ACRYREX® CM-207

Product Description: Medium viscosity
PropertiesISO Test MethodTest ConditionUnitCM-207
Melt Flow Index1133 230℃×3.8KGml/10 min8.5 
Mass Density1183 23 ℃g/cm31.19 
Tensile Strength527 5 mm/min, yieldMPa67 
50 mm/min, breakMPa67 
Tensile Elongation527 50 mm/min%
Flexural Strength178 2 mm/minMPa97 
Flexural Modulus2 mm/minGPa2.7 
Izod Impact Strength180/1A23℃, NotchedKJ/m2
-30℃, NotchedKJ/m2
Charpy Impact Strength179 23℃, NotchedKJ/m2
Charpy
‘-30℃, Notched
KJ/m2
Vicat Softening Temp.306 50℃/hr;1KG107 
50℃/hr;5KG99 
Heat Distortion Temp.75/A1.8MPa, unannealed89 
1.8MPa, annealed100 
Coefficient of Linear
Thermal Expansion
11359 6 X 10-5
FlammabilityUL-941.5mm HB
Mold Shrinkage294-4%0.2~0.6
Symbol1043 >PMMA<
August 23, 2023
Notes:These are typical properties only and are not to be construed as specifications. Users
should confirm results by their own test

Acryrex® CM-207 UL Product iQ

ACRYREX® CM-207 | UL Product iQ
File Number: E56070Yellow Card™Polymethyl Methacrylate (PMMA) “ACRYREX”, furnished as pellets
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLHB
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLHB75
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)PLC 4UL 746A
(1.5 mm)
High Amp Arc Ignition (HAI)PLC 0UL 746A
(1.5 mm)
Comparative Tracking Index (CTI)PLC 1UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 0
High Voltage, Low Current Arc ResistancePLC 6
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm50   °C
3.0 mm50   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm50   °C
3.0 mm50   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm50   °C
3.0 mm50   °C
Report Date: 1982-06-22

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top