Chimei ACRYREX® CM-211 PMMA

ACRYREX® PMMA Resin CM-211

ACRYREX® CM-211 PMMA Transparent Grade High Flow


Chimei ACRYREX CM-211 PMMA resin is a high-flow, low-viscosity material designed for precision molding. Ideal for intricate parts in home appliances and daily necessities, it combines superior processability with durability, heat resistance, and compliance with safety standards like UL 94 HB.

  • Manufacturer: CHIMEI
  • Packaging: 25kg bag
  • Character: High flow/Processability
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data (ISO)

  • Flow Efficiency: 16 ml/10 min (ISO 1133)
  • Mechanical Strength: 65 MPa tensile, 95 MPa flexural
  • Heat Tolerance: 103°C Vicat
  • Safety Compliance: UL 94 HB flammability rating
  • Low Shrinkage: 0.2–0.6%

Superior Flow for Complex Molds

With a melt flow index of 16 ml/10 min (230°C, 3.8kg), ACRYREX CM-211 PMMA fills intricate molds effortlessly, reducing cycle times and minimizing defects in thin-walled or detailed components like appliance housings.

Robust Strength for Durable Parts

Boasting 65 MPa tensile strength and 95 MPa flexural strength, this PMMA acryrex CM-211 resists cracking and deformation, ensuring long-lasting performance in high-stress applications such as transparent covers or kitchen utensils.

Heat Resistance for Stable Performance

A Vicat softening temperature of 103°C (1kg) allows PMMA CM-211 to withstand repeated exposure to heat, making it ideal for dishwasher-safe items or components near heat sources in appliances.

ACRYREX PMMA Resin CM-211

Applications

  • Home Appliance Parts: Transparent microwave turntables, blender jars, and refrigerator compartments.
  • Daily Necessities: Shatter-resistant cosmetic containers, bathroom accessories, and kitchenware.
  • Electronics: Light diffusers, control panels, and touch-sensitive covers requiring clarity and toughness.
Chimei ACRYREX PMMA Resin CM-211 Application

Acryrex® CM-211 Datasheet

General PMMA ACRYREX® CM-211

Product Description: Low viscosity
PropertiesISO Test MethodTest ConditionUnitCM-211
Melt Flow Index1133 230℃×3.8KGml/10 min16 
Mass Density1183 23 ℃g/cm31.19 
Tensile Strength527 5 mm/min, yieldMPa65 
50 mm/min, breakMPa65 
Tensile Elongation527 50 mm/min%
Flexural Strength178 2 mm/minMPa95 
Flexural Modulus2 mm/minGPa2.7 
Izod Impact Strength180/1A23℃, NotchedKJ/m2
-30℃, NotchedKJ/m2
Charpy Impact Strength179 23℃, NotchedKJ/m2
Charpy
‘-30℃, Notched
KJ/m2
Vicat Softening Temp.306 50℃/hr;1KG103 
50℃/hr;5KG96 
Heat Distortion Temp.75/A1.8MPa, unannealed78 
1.8MPa, annealed98 
Coefficient of Linear
Thermal Expansion
11359 6 X 10-5
FlammabilityUL-941.5mm HB
Mold Shrinkage294-4%0.2~0.6
Symbol1043 >PMMA<
August 23, 2023
Notes:These are typical properties only and are not to be construed as specifications. Users
should confirm results by their own test

Acryrex® CM-211 UL Product iQ

ACRYREX® CM-211 | UL Product iQ
File Number: E56070Yellow Card™Polymethyl Methacrylate (PMMA) “ACRYREX”, furnished as pellets
(v) – Vicat softening temperature of 95 degree C achieved at 3.0mm
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLHB
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLHB75
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.5 mmPLC 4
3.0 mmPLC 3
High Amp Arc Ignition (HAI)PLC 0UL 746A
(1.5 mm)
Comparative Tracking Index (CTI)PLC 1UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 0
High Voltage, Low Current Arc ResistancePLC 6
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm50   °C
3.0 mm50   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm50   °C
3.0 mm50   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm50   °C
3.0 mm50   °C
Report Date: 1982-06-22

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top