Sinochem Fuya® HD55110 HDPE

Sinochem HDPE resin

Sinochem HDPE HD55110 Plastic Transport Container

Sinochem HD55110 is a premium bimodal titanium-catalyzed HDPE resin engineered for high-performance film applications. With exceptional rigidity, superior sealing performance, and excellent processability, it ensures consistent quality in high-speed production.

  • Manufacturer: Sinochem Quan Zhou Petrochemical Co., Ltd.
  • Character: Bimodal Titanium-Catalyzed Product
  • Application: packaging solutions like shopping bags, food bags, and industrial films
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (GB/T)

  • Density: 0.9545 g/cm³
  • Melt Flow Rate: 8.85 g/10min
  • Tensile Strength: 27.1 MPa
  • Elongation at Break: 639%
  • Fish Eye Count: ≤3
  • Impact Strength: 122.5 g


High-Speed Processability

Sinochem HDPE resin HD55110 offers a melt flow rate of 8.85 g/10min, enabling faster extrusion and reduced energy consumption. Perfect for high-output film production lines.

Unmatched Durability

With tensile strength of 27.1 MPa and elongation at 639%, this resin creates tear-resistant films. Ideal for heavy-duty garbage bags or reusable shopping bags.

Flawless Surface Quality

Zero black/color particles and minimal fish eyes (3/1520cm²) ensure pristine printability and clarity, critical for branded food packaging or pharmaceutical films.

Sinochem HDPE resin pellets

Application

  • Retail & Consumer: Vest bags, shopping bags, branded packaging films.
  • Food Safety: Leak-proof food bags, transparent beverage films.
  • Industrial: Heavy-duty garbage bags, pharmaceutical blister packaging.
  • Logistics: Protective films for bottled products and fragile items.
Sinochem HDPE HD55110 application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity