LG PC1300-10 General Purpose Grade
LG Chem PC1300-10 is a high-performance polycarbonate resin designed for injection molding. It delivers an exceptional balance of high impact strength, outstanding transparency, and excellent coloring properties for demanding applications.
- Character: Coloring, High Impact Resistance, High Transparency
- Application: Others, Sheet/Flim
Key technical data
- Melt Flow Rate (300°C/1.2 kg): 10 g/10min
- Light Transmittance: 89%
- Haze: 0.7 – 1.5%
- Notched Izod Impact (@ 23°C): 900 J/m
- Tensile Yield Strength: 60 MPa
- Flexural Modulus: 2410 MPa
- Deflection Temperature (1.8 MPa, Annealed): 141 °C
- UL-94 Flame Class (1.6 mm): V-2
Application
- Protective Sight Glasses and Covers
- TransMachine Guards and Shields
- High-Clarity Film and Sheet
- Components for Electronics Housings
- Decorative and Functional Panels
Features & Benefits

Related LG PC Resin Products