Yulong A-2020 ABS Resin

Yulong ABS Resin Plastic Raw material

Yulong A-2020 General Purpose Grade

Yulong A-2020 is a high-performance ABS resin pellet offering excellent impact strength, rigidity, and thermal stability. It is widely suitable for injection molding processes, making it an ideal material choice for applications such as electronic housings, home appliances, and automotive components.

  • Character: excellent impact strength, rigidity, and thermal stability
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Melt Flow Rate (10kg, 220°C): 19.1 g/10min
  • Izod Impact Strength (1/4″” notch): 21 kg·cm/cm
  • Rockwell Hardness (R Scale): 111
  • Tensile Strength: 46.3 MPa
  • Flexural Strength: 65.8 MPa
  • Flexural Modulus: 2400 MPa
  • Vicat Softening Temperature (B50): 94.4°C
  • Whiteness Index: 59.2%
  • Yellowness Index: 8.0

Application

  • Electronic device housings
  • Household appliance components
  • Automotive interior parts
  • Consumer goods and office equipment
  • Toys and sports equipment

Features & Benefits

High Impact Resistance

Notched Izod impact strength of 21 kg·cm/cm helps prevent cracking during transport or use, extending product life.

Excellent Rigidity

Flexural modulus of 2400 MPa and Rockwell hardness of 111 ensure dimensional stability and strong load-bearing capacity, ideal for structural parts.

Excellent Processability

Melt flow rate of 19.1 g/10min enables easy injection molding with short cycle times, suitable for complex-shaped products.

Acrylonitrile Butadiene Styrene ABS Resin

Related Yulong ABS Granules

Advanced Manufacturing