Juyuan JY-PC-920UR is a high-performance Polycarbonate (PC) resin granule offering excellent UV resistance, good flow properties, and easy release characteristics. Suitable for injection molding, it is widely used in various general plastic applications, delivering outstanding durability and stability for both indoor and outdoor products.

  • Character: Low viscosity, Anti-UV Grade, Flammability HB V-2, easy release
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Melt Flow Rate (300°C, 1.2kg): 20.0 g/10min
  • Tensile Strength: 65 MPa
  • Flexural Strength: 94 MPa
  • Izod Impact Strength (Notched): 70 J/m² (ASTM D256)
  • Water Absorption: 0.30%
  • HDT (1.8MPa): 124 °C
  • Flammability Rating: 0.75mm – 2.4mm: V-2
  • Flammability Rating: 2.5mm – 6.0mm: HB
  • Light Transmittance (1000µm): 90.50%

Application

  • Electronic and electrical enclosures
  • Automotive light covers and interior components
  • Outdoor lighting fixtures
  • Home appliance parts
  • General industrial components
  • Structural parts for consumer electronics

Features & Benefits

UV Resistance

Formulated with UV stabilizers to resist degradation from long-term outdoor exposure, extending product lifespan.

Easy Release

It contains a release agent to improve mold release efficiency, reduce cycle times, and enable high-volume production.

Flame Retardant

Compliant with UL 94 V-2 and HB ratings across multiple thicknesses, ensuring safety for various applications.

Polycarbonate PC Resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top