Chimei Polylac® PA-709
Polylac® PA-709 Super Impact General ABS Resin Polylac PA-709 is a high-performance ABS material used in medical and industrial applications. It offers low monomer residue (EU 10/2011) and ISO10993 biocompatibility. With high impact strength (37 kJ/m²) and tensile strength (40 MPa), it is durable even in cold conditions. Easy to mold at 220°C and with