PC Resin

LEXAN™ PC Resin 143R

SABIC PC Lexan 143R General Purpose Grade SABIC Lexan 143R is a versatile, UV-stabilized polycarbonate resin. It offers an excellent balance of high impact strength, clarity, and ease of processing with a built-in mold release, ideal for demanding applications across various industries. Key technical data Download Application Features & Benefits Related Lexan™ Polycarbonate Products Advanced

LEXAN™ PC Resin 143R Read More »

LEXAN™ PC Resin 141R

SABIC PC Lexan 141R General Purpose Grade SABIC Lexan 141R is a versatile 11 MFR polycarbonate resin featuring internal mold release for high-efficiency processing and a UL94 HB flame rating, ideal for durable components. Key technical data Download Application Features & Benefits Related Lexan™ Polycarbonate Products Advanced Manufacturing

LEXAN™ PC Resin 141R Read More »

LEXAN™ PC Resin 123R

SABIC PC Lexan 123R General Purpose Grade SABIC Lexan 123R is a versatile, high-performance polycarbonate resin. This 18 MFR material is UV stabilized, contains a mold release, and carries key UL ratings for electrical and flame safety. Key technical data Download Application Features & Benefits Related Lexan™ Polycarbonate Products Advanced Manufacturing

LEXAN™ PC Resin 123R Read More »

LEXAN™ PC Resin 121R

SABIC PC Lexan 121R General Purpose Grade SABIC Lexan 121R is an 18 MFR polycarbonate resin featuring mold release for easy processing and a UL94 HB flame rating. It delivers an exceptional balance of impact strength, clarity, and thermal resistance for demanding applications. Key technical data Download Application Features & Benefits Related Lexan™ Polycarbonate Products

LEXAN™ PC Resin 121R Read More »

LEXAN™ PC Resin Sabic Tianjin

LEXAN™ PC Resin 101

Lexan 101 general Purpose Grade Lexan PC Resin 101 is a versatile 7 MFR polycarbonate, ideal for both extrusion and injection molding. It offers an outstanding balance of high impact strength, clarity, and thermal resistance, perfect for demanding industrial applications. Key technical data Download Application Features & Benefits Related Lexan™ Polycarbonate Products Advanced Manufacturing

LEXAN™ PC Resin 101 Read More »

LEXAN™ PC Resin 103R

SABIC PC Lexan 103R General Purpose Grade SABIC Lexan 103R is a versatile, UV-stabilized polycarbonate resin. It features mold release for easier processing and carries key UL ratings (94HB, 746C F1), making it a reliable, high-performance choice for demanding applications. Key technical data Download Application Features & Benefits Related Lexan™ Polycarbonate Products Advanced Manufacturing

LEXAN™ PC Resin 103R Read More »

Juyuan PC Resin JY-PC-920UR

Juyuan JY-PC-920UR General Purpose Grade Juyuan JY-PC-920UR is a high-performance Polycarbonate (PC) resin granule offering excellent UV resistance, good flow properties, and easy release characteristics. Suitable for injection molding, it is widely used in various general plastic applications, delivering outstanding durability and stability for both indoor and outdoor products. Key technical data Download Application Features

Juyuan PC Resin JY-PC-920UR Read More »

Juyuan PC Resin JY-PC-910UR

Juyuan JY-PC-910UR General Purpose Grade Juyuan JY-PC-910UR is a medium-viscosity, UV-resistant polycarbonate resin granule designed for injection molding. It offers excellent mechanical strength, high light transmittance, and good flame retardancy, making it ideal for general plastic applications—especially those requiring weatherability and stability in outdoor and electronic uses. Key technical data Download Application Features & Benefits

Juyuan PC Resin JY-PC-910UR Read More »

Juyuan PC Resin JY-PC-910RB

Juyuan JY-PC-910RB General Purpose Grade Juyuan JY-PC-910RB is a medium-viscosity Polycarbonate (PC) resin granule offering excellent transparency, high impact strength, and good flame retardancy (HB/V-2). Ideal for injection molding, it is widely used in general plastic applications, combining easy release with high production efficiency. Key technical data Download Application Features & Benefits Related Juyuan polycarbonate

Juyuan PC Resin JY-PC-910RB Read More »

SABIC® PC Resin PC5800

Sabic PC Resin PC5800 Injection Molding Grade Sabic PC5800 is a very high flow polycarbonate, ideal for optical media and complex, thin-walled components requiring superior clarity and process efficiency. Key technical data Download Application Features & Benefits Related Sabic® Polycarbonate Products Advanced Manufacturing

SABIC® PC Resin PC5800 Read More »