Polylac® PA-709 Super Impact General ABS Resin
Polylac PA-709 is a high-performance ABS material used in medical and industrial applications. It offers low monomer residue (EU 10/2011) and ISO10993 biocompatibility. With high impact strength (37 kJ/m²) and tensile strength (40 MPa), it is durable even in cold conditions. Easy to mold at 220°C and with UL94 HB flammability standards, it is ideal for medical, electrical, or durable parts.
- Application: Plumbing fittings/front and rear vehicle spoiler/motorcycle fenders/safety helmets/water filter casings
- Character: Ultra high impact strength/good low temperature resistance
Download
Access essential product documentation including technical data sheets, safety information, environmental certifications, and processing guides.
All documents are sourced directly from manufacturers and updated regularly for accuracy.


Polylac® PA-709 Datasheet
| General ABS POLYLAC® PA-709 | ||||
| Product Description: Super impact | ||||
| Properties | ISO Test Method | Test Condition | Unit | PA-709 |
| Melt Flow Index | 1133 | 220℃×10KG | ml/10 min | 6 |
| Mass Density | 1183 | 23 ℃ | g/cm3 | 1.03 |
| Tensile Strength | 527 | 50 mm/min, yield | MPa | 40 |
| 50 mm/min, break | MPa | 31 | ||
| Tensile Elongation | 527 | 50 mm/min | % | 35 |
| Flexural Strength | 178 | 2 mm/min | MPa | 58 |
| Flexural Modulus | 178 | 2 mm/min | GPa | 1.8 |
| Izod Impact Strength | 180/1A | 23℃, Notched | KJ/m2 | 37 |
| -30℃, Notched | KJ/m2 | 27 | ||
| Charpy Impact Strength | 179 | 23℃, Notched | KJ/m2 | 38 |
| -30℃, Notched | KJ/m2 | 29 | ||
| Vicat Softening Temp. | 306 | 50℃/hr;1KG | ℃ | 105 |
| 50℃/hr;5KG | ℃ | 97 | ||
| Heat Distortion Temp. | 75/A | 1.8MPa, unannealed | ℃ | 82 |
| 1.8MPa, annealed | ℃ | 98 | ||
| Coefficient of Linear Thermal Expansion | 11359 | – | – | 9.3 x 10-5 |
| Flammability | – | UL-94 | – | 1.5mm HB |
| Mold Shrinkage | 294-4 | – | % | 0.4~0.7 |
| Symbol | 1043 | – | – | >ABS< |
| March 11, 2024 | ||||
Polylac® PA-709 UL Product iQ
| POLYLAC® PA-709 UL Product iQ | ||
| File Number: E56070 | Yellow Card™ | Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets |
| FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | ANSI/UL 94 | |
| 1.5 mm, Color: ALL | HB | |
| 3.0 mm, Color: ALL | HB | |
| ISO/IEC FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | IEC 60695-11-10 | |
| 1.5 mm, Color: ALL | HB75 | |
| 3.0 mm, Color: ALL | HB40 | |
| ELECTRICAL PROPERTIES | VALUE | TEST METHOD |
| Hot-wire Ignition (HWI) | UL 746A | |
| 1.5 mm | PLC 4 | |
| 3.0 mm | PLC 4 | |
| High Amp Arc Ignition (HAI) | UL 746A | |
| 1.5 mm | PLC 0 | |
| 3.0 mm | PLC 0 | |
| Comparative Tracking Index (CTI) | PLC 1 | UL 746A |
| High Voltage Arc Tracking Rate (HVTR) | PLC 0 | |
| High Voltage, Low Current Arc Resistance | PLC 6 | |
| THERMAL PROPERTIES | VALUE | TEST METHOD |
| Relative Thermal Index – Electrical Strength | UL 746B | |
| 1.5 mm | 60 °C | |
| 3.0 mm | 60 °C | |
| Relative Thermal Index – Mechanical Impact | UL 746B | |
| 1.5 mm | 60 °C | |
| 3.0 mm | 60 °C | |
| Relative Thermal Index – Mechanical Strength | UL 746B | |
| 1.5 mm | 60 °C | |
| 3.0 mm | 60 °C | |
| Report Date: 1983-06-23 | ||