Polylac® PA-709s Super Impact General ABS Resin
Polylac PA-709S is a high-impact ABS resin that boasts excellent strength and durability. It’s ideal for making pipe materials, appliances, and large containers. With good tensile strength and easy processing, Polylac PA-709S ensures reliable performance across various applications.
- Application: Pipe materials/appliances/large containers
- Character: Ultra-high impact resistance
Download
Access essential product documentation including technical data sheets, safety information, environmental certifications, and processing guides.
All documents are sourced directly from manufacturers and updated regularly for accuracy.


Polylac® PA-709S Datasheet
| Extrusion ABS POLYLAC® PA-709S | ||||
| Product Description: Super impact Extrusion | ||||
| Properties | ISO Test Method | Test Condition | Unit | PA-709S |
| Melt Flow Index | 1133 | 220℃×10KG | ml/10 min | 4 |
| Mass Density | 1183 | 23 ℃ | g/cm3 | 1.03 |
| Tensile Strength | 527 | 50 mm/min, yield | MPa | 37 |
| 50 mm/min, break | MPa | 29 | ||
| Tensile Elongation | 527 | 50 mm/min | % | 35 |
| Flexural Strength | 178 | 2 mm/min | MPa | 51 |
| Flexural Modulus | 178 | 2 mm/min | GPa | 1.5 |
| Izod Impact Strength | 180/1A | 23℃, Notched | KJ/m2 | 40 |
| -30℃, Notched | KJ/m2 | 28 | ||
| Charpy Impact Strength | 179 | 23℃, Notched | KJ/m2 | 42 |
| -30℃, Notched | KJ/m2 | 30 | ||
| Vicat Softening Temp. | 306 | 50℃/hr;1KG | ℃ | 104 |
| 50℃/hr;5KG | ℃ | 98 | ||
| Heat Distortion Temp. | 75/A | 1.8MPa, unannealed | ℃ | 81 |
| 1.8MPa, annealed | ℃ | 96 | ||
| Coefficient of Linear Thermal Expansion | 11359 | – | – | 9.5 x 10-5 |
| Flammability | – | UL-94 | – | 1.5mm HB |
| Mold Shrinkage | 294-4 | – | % | 0.4~0.7 |
| Symbol | 1043 | – | – | >ABS< |
| March 11, 2024 | ||||
Polylac® PA-709S UL Product iQ
| POLYLAC® PA-709S UL Product iQ | ||
| File Number: E56070 | Yellow Card™ | Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets |
| FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | ANSI/UL 94 | |
| 1.5 mm, Color: ALL | HB | |
| 3.0 mm, Color: ALL | HB | |
| ISO/IEC FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | IEC 60695-11-10 | |
| 1.5 mm, Color: ALL | HB75 | |
| 3.0 mm, Color: ALL | HB40 | |
| ELECTRICAL PROPERTIES | VALUE | TEST METHOD |
| Hot-wire Ignition (HWI) | UL 746A | |
| 1.5 mm | PLC 4 | |
| 3.0 mm | PLC 2 | |
| High Amp Arc Ignition (HAI) | UL 746A | |
| 1.5 mm | PLC 0 | |
| 3.0 mm | PLC 0 | |
| Comparative Tracking Index (CTI) | PLC 0 | UL 746A |
| High Voltage Arc Tracking Rate (HVTR) | PLC 0 | |
| High Voltage, Low Current Arc Resistance | PLC 7 | |
| THERMAL PROPERTIES | VALUE | TEST METHOD |
| Relative Thermal Index – Electrical Strength | UL 746B | |
| 1.5 mm | 60 °C | |
| 3.0 mm | 60 °C | |
| Relative Thermal Index – Mechanical Impact | UL 746B | |
| 1.5 mm | 60 °C | |
| 3.0 mm | 60 °C | |
| Relative Thermal Index – Mechanical Strength | UL 746B | |
| 1.5 mm | 60 °C | |
| 3.0 mm | 60 °C | |
| Report Date: 1983-06-23 | ||