Chimei Polylac® PA-717C ABS

Chimei POLYLAC PA-717C ABS Resin

Polylac® PA-717C General Grade High Impact Strength


Polylac PA-717C ABS resin delivers high impact strength and durability for demanding industrial applications.This general-purpose ABS combines toughness with thermal stability (Vicat 103°C) and smooth molding efficiency.

  • Application: Kitchen appliances, audio supplies, toilet seats, washing machines, vacuum cleaner housings, tool handle accessories
  • Character: High impact strength
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Impact Strength: 25 KJ/m² (23°C, Izod) | 12 KJ/m² (-30°C)
  • Thermal Resistance: Vicat 103°C (1KG) | HDT 97°C (annealed)
  • Flammability: UL94 HB (1.5mm) – Safe for consumer goods.
  • Mold Shrinkage: 0.4–0.7% – Tight tolerances for precision parts.
  • Electrical Properties: CTI PLC 1 – Suitable for electronic housings.

Exceptional Impact Resistance

POLYLAC PA-717C offers 25 KJ/m² Izod Impact Strength (23°C), reducing cracks in high-stress parts like vacuum cleaner housings or tool handles. Ensures longevity in rugged environments.

Reliable Heat Stability

It can withstand temperatures up to 103°C (Vicat Softening) and 97°C Heat Distortion (annealed), preventing warping in kitchen appliances or washing machine components during prolonged use.

Optimized Molding Efficiency

A Melt Flow Index of 17 ml/10 min ensures smooth flow into intricate molds, reducing cycle times for complex designs like audio equipment or toilet seats.

Chimei POLYLAC PA-717C ABS

Applications

  • Kitchen Appliances: Blenders, coffee makers (heat resistance + smooth finish).
  • Vacuum Cleaner Housings: Lightweight yet crack-resistant.
  • Toilet Seats: Easy-to-clean surface and structural integrity.
  • Tool Handles: Ergonomically molded for shock absorption.
  • Audio Equipment: Sleek, high-gloss finishes.
  • Washing Machines: Durable panels resistant to steam and impact.
Chimei POLYLAC PA-717C application

Polylac® PA-717C Datasheet

General ABS POLYLAC®  PA-717C
Product Description: Medium impact
PropertiesISO Test MethodTest ConditionUnitPA-717C
Melt Flow Index1133 220℃×10KGml/10 min17 
Mass Density1183 23 ℃g/cm31.04 
Tensile Strength527 50 mm/min, yieldMPa44 
50 mm/min, breakMPa33 
Tensile Elongation527 50 mm/min%45 
Flexural Strength178 2 mm/minMPa69 
Flexural Modulus2 mm/minGPa1.9 
Izod Impact Strength180/1A23℃, NotchedKJ/m225 
-30℃, NotchedKJ/m212 
Charpy Impact Strength179 23℃, NotchedKJ/m227 
-30℃, NotchedKJ/m213 
Vicat Softening Temp.306 50℃/hr;1KG103 
50℃/hr;5KG98 
Heat Distortion Temp.75/A1.8MPa, unannealed82 
1.8MPa, annealed97 
Coefficient of Linear Thermal Expansion11359 8.8 x 10-5
FlammabilityUL-941.5mm HB
Mold Shrinkage294-4%0.4~0.7
Symbol1043 >ABS<
March  12, 2025
Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test.

Polylac® PA-717C UL Product iQ

POLYLAC® PA-717C(+) | UL Product iQ
File Number: E56070Yellow Card™Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets
(+) – Indicate 0~0.5% acid scavengers.
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLHB
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLHB75
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.5 mmPLC 4
3.0 mmPLC 4
High Amp Arc Ignition (HAI)UL 746A
1.5 mmPLC 1
3.0 mmPLC 0
Comparative Tracking Index (CTI)PLC 1UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 0
Volume Resistivity1.0E+16   ohms·cmASTM D257/IEC 60093
High Voltage, Low Current Arc ResistancePLC 7
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm85   °C
3.0 mm85   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm80   °C
3.0 mm80   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm85   °C
3.0 mm85   °C

Related Polylac® ABS Plastics

No post found!

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top