POLYLAC PA-746M is a high-flow ABS resin engineered for large, complex parts requiring flawless painting. With exceptional processability and adhesion, it’s ideal for automotive and consumer goods. Whether you’re molding automotive parts or consumer goods, this resin ensures efficiency without compromise.

  • Application: Paintable two wheeler application
  • Character: High flowability, high impact strength
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 50 ml/10 min
  • Tensile Strength (Yield): 41 MPa
  • Izod Impact (23°C): 19 KJ/m²
  • Vicat Softening Temp.: 104°C (1KG load)
  • Mold Shrinkage: 0.4–0.7%
  • Flammability Rating: UL94 HB (1.5mm)
  • Certifications: UL Recognized

Superior Mold-Filling Efficiency

POLYLAC PA-746H’s high melt flow index (40 ml/10 min) ensures rapid, uniform filling of intricate molds—ideal for thin-wall designs like automotive trim or electronics housings, reducing cycle times and material waste.

Reliable Impact Resistance

With Izod impact strength of 27 KJ/m² (23°C) and 12 KJ/m² (-30°C), this ABS resin withstands drops, vibrations, and cold environments, perfect for outdoor equipment or automotive components exposed to harsh conditions.

Thermal Stability Under Pressure

A Vicat softening temperature of 102°C (1KG load) ensures dimensional stability during high-heat processes like plating or assembly, minimizing warping in appliances or industrial parts.

Chimei POLYLAC PA-746M ABS

Applications

  • Motorcycle fairings and side panels.
  • Scooter body kits with glossy finishes.
  • Helmets and visors requiring scratch-resistant coatings.
  • All-terrain vehicle (ATV) trim and fenders.
Chimei POLYLAC PA-746M application

Polylac® PA-746M Datasheet

Painting ABS POLYLAC®  PA-746M
Product Description: Excellent Processability and Adhesion Properties
PropertiesISO Test MethodTest ConditionUnitPA-746M
Melt Flow Index1133 220℃×10KGml/10 min50 
Mass Density1183 23 ℃g/cm31.04 
Tensile Strength527 50 mm/min, yieldMPa41 
50 mm/min, breakMPa30 
Tensile Elongation527 50 mm/min%50 
Flexural Strength178 2 mm/minMPa61 
Flexural Modulus2 mm/minGPa2.1 
Izod Impact Strength180/1A23℃, NotchedKJ/m219 
-30℃, NotchedKJ/m2
Charpy Impact Strength179 23℃, NotchedKJ/m220 
-30℃, NotchedKJ/m2
Vicat Softening Temp.306 50℃/hr;1KG104 
50℃/hr;5KG99 
Heat Distortion Temp.75/A1.8MPa, unannealed
1.8MPa, annealed96 
Coefficient of Linear Thermal Expansion11359 8.3 x 10-5
FlammabilityUL-941.5mm HB
Mold Shrinkage294-4%0.4~0.7
Symbol1043 >ABS<
March  12, 2025
Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test

Polylac® PA-746M UL Product iQ

POLYLAC® PA-746M | UL Product iQ
File Number: E56070Yellow Card™Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLHB
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLHB75
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.5 mmPLC 5
3.0 mmPLC 5
High Amp Arc Ignition (HAI)UL 746A
1.5 mmPLC 1
3.0 mmPLC 1
Comparative Tracking Index (CTI)PLC 1UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 3
High Voltage, Low Current Arc ResistancePLC 7
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm60   °C
3.0 mm60   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm60   °C
3.0 mm60   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm60   °C
3.0 mm60   °C

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top