Polylac® PA-747R Extrusion Grade High Impact Strength
Polylac PA-747R ABS resin is a high-impact extrusion-grade material engineered for durability and thermal stability. Ideal for luggage, refrigerator plating, and industrial profiles, it combines smooth processing with exceptional strength, even in extreme temperatures.
- Character: High impact strength profile extrusion materials
Key technical data (ISO)
- Melt Flow Index: 2.5 ml/10 min (220°C, 10kg)
- Impact Strength: 37 KJ/m² (23°C) / 26 KJ/m² (-30°C)
- Thermal Stability: Vicat 106°C / HDT up to 99°C
- Flammability: UL94 HB (1.5mm)
- Mold Shrinkage: 0.4–0.7%

Applications
- Extrusion Materials: Automotive trims, window seals, and industrial profiles requiring consistent finish.
- Luggage/Suitcases: Lightweight yet impact-resistant shells for travel gear.
- Refrigerator Plating: Glossy, heat-resistant surfaces that maintain aesthetics in appliances.

Polylac® PA-747R Datasheet
| Extrusion ABS POLYLAC® PA-747R Product Description: Extrusion | ||||
| Properties | ISO Test Method | Test Condition | Unit | PA-747R |
| Melt Flow Index | 1133 | 220℃×10KG | ml/10 min | 2.5 |
| Mass Density | 1183 | 23 ℃ | g/cm3 | 1.04 |
| Tensile Strength | 527 | 50 mm/min, yield | MPa | 41 |
| 50 mm/min, break | MPa | 30 | ||
| Tensile Elongation | 527 | 50 mm/min | % | 30 |
| Flexural Strength | 178 | 2 mm/min | MPa | 61 |
| Flexural Modulus | 2 mm/min | GPa | 1.7 | |
| Izod Impact Strength | 180/1A | 23℃, Notched | KJ/m2 | 37 |
| -30℃, Notched | KJ/m2 | 26 | ||
| Charpy Impact Strength | 179 | 23℃, Notched | KJ/m2 | 39 |
| -30℃, Notched | KJ/m2 | 28 | ||
| Vicat Softening Temp. | 306 | 50℃/hr;1KG | ℃ | 106 |
| 50℃/hr;5KG | ℃ | 99 | ||
| Heat Distortion Temp. | 75/A | 1.8MPa, unannealed | ℃ | 83 |
| 1.8MPa, annealed | ℃ | 99 | ||
| Coefficient of Linear Thermal Expansion | 11359 | – | – | 9.1 x 10-5 |
| Flammability | – | UL-94 | – | 1.5mm HB |
| Mold Shrinkage | 294-4 | – | % | 0.4~0.7 |
| Symbol | 1043 | – | – | >ABS< |
| March 12, 2025 Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test | ||||
Polylac® PA-747R UL Product iQ
| POLYLAC® PA-747R | UL Product iQ | ||
| File Number: E56070 | Yellow Card™ | Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets |
| FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | ANSI/UL 94 | |
| 1.5 mm, Color: ALL | HB | |
| 3.0 mm, Color: ALL | HB | |
| ISO/IEC FLAMMABILITY PROPERTIES | VALUE | TEST METHOD |
| Flammability | IEC 60695-11-10 | |
| 1.5 mm, Color: ALL | HB75 | |
| 3.0 mm, Color: ALL | HB40 | |
| ELECTRICAL PROPERTIES | VALUE | TEST METHOD |
| Hot-wire Ignition (HWI) | UL 746A | |
| 1.5 mm | PLC 4 | |
| 3.0 mm | PLC 4 | |
| High Amp Arc Ignition (HAI) | UL 746A | |
| 1.5 mm | PLC 0 | |
| 3.0 mm | PLC 0 | |
| Comparative Tracking Index (CTI) | PLC 1 | UL 746A |
| High Voltage Arc Tracking Rate (HVTR) | PLC 0 | |
| High Voltage, Low Current Arc Resistance | PLC 6 | |
| THERMAL PROPERTIES | VALUE | TEST METHOD |
| Relative Thermal Index – Electrical Strength | UL 746B | |
| 1.5 mm | 60 °C | |
| 3.0 mm | 60 °C | |
| Relative Thermal Index – Mechanical Impact | UL 746B | |
| 1.5 mm | 60 °C | |
| 3.0 mm | 60 °C | |
| Relative Thermal Index – Mechanical Strength | UL 746B | |
| 1.5 mm | 60 °C | |
| 3.0 mm | 60 °C | |