LG Chem PC1300-10

LG Chem PC Polycarbonate

LG PC1300-10 General Purpose Grade

LG Chem PC1300-10 is a high-performance polycarbonate resin designed for injection molding. It delivers an exceptional balance of high impact strength, outstanding transparency, and excellent coloring properties for demanding applications.

  • Character: Coloring, High Impact Resistance, High Transparency
  • Application: Others, Sheet/Flim
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Melt Flow Rate (300°C/1.2 kg): 10 g/10min
  • Light Transmittance: 89%
  • Haze: 0.7 – 1.5%
  • Notched Izod Impact (@ 23°C): 900 J/m
  • Tensile Yield Strength: 60 MPa
  • Flexural Modulus: 2410 MPa
  • Deflection Temperature (1.8 MPa, Annealed): 141 °C
  • UL-94 Flame Class (1.6 mm): V-2

Application

  • Protective Sight Glasses and Covers
  • TransMachine Guards and Shields
  • High-Clarity Film and Sheet
  • Components for Electronics Housings
  • Decorative and Functional Panels

Features & Benefits

Superior Impact Resistance

With an exceptional Notched Izod Impact strength, LG PC1300-10 withstands sudden impacts and harsh handling, reducing part failure and ensuring product longevity in tough environments.

Crystal-Clear Transparency

This material offers high light transmittance and low haze, providing brilliant optical clarity ideal for displays, covers, and any application where visual appeal and see-through quality are critical.

Reliable Flame Retardancy

The LG PC1300-10 resin complies with UL94 V-2 ratings at various thicknesses, offering vital flame retardancy for components in electronics and electrical equipment, enhancing end-product safety.

LG Chem ABS Plastic Raw Material General Purpose

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine