Sinochem Fuya® H3030F

Sinochem PP resin

Sinochem PP H3030F High Stiffness Ultra-Clear BOPP Films

Sinochem H3030F is a premium homopolymer polypropylene (PP) resin engineered for BOPP films. With excellent film-forming properties, high stiffness, and crystal-clear transparency, it’s ideal for high-value packaging like glossy, matte, and pearlescent films. Trusted for consistency and purity, Sinochem PP resin delivers performance that meets rigorous industrial demands.

  • Character: High Rigidity, Exceptional Transparency, Superior Processability, Pristine Purity
  • Application: high-value packaging like glossy, matte, and pearlescent films.
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (GB/T)

  • Melt Flow Rate (230°C/2.16kg): 3.11 g/10min
  • Tensile Strength: 31.8 MPa
  • Isotactic Index: 96.1%
  • Yellow Index: -2.78
  • Impurity Control: 0 fish eye/1520cm², 3 color particles/kg


High Durable Films

Sinochem H3030F boasts a tensile yield stress of 31.8 MPa, exceeding industry standards. This ensures films resist tearing and maintain structural integrity, even in high-speed packaging lines.

Exceptional Clarity

With a yellow index of -2.78 (far below the 4.0 limit), this PP resin produces films with unmatched transparency. Perfect for showcasing products in food, cosmetics, or luxury packaging.

Stable Melt Flow

The melt flow rate of 3.11 g/10min ensures smooth extrusion and uniform thickness, reducing waste and downtime in BOPP film production.

Sinochem PP resin pellets

Application

  • High-gloss packaging films (e.g., snack bags, candy wrappers).
  • Matte-finish labels for premium cosmetics or beverages.
  • Pearlescent films in luxury gift packaging.
  • Lightweight yet rigid films for industrial lamination.
Sinochem HDPE QZF144 application

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top