Chimei Polylac® PA-763 ABS

Chimei Polylac ABS Resin PA-763

Polylac® PA-763 Flame Retardant High Impact ABS

Polylac PA-763 ABS Resin is a high-performance, flame-retardant material designed for safety and durability. It meets 1.5mm V-0 and 2.5mm 5VA fire safety standards (UL-94). Its high impact strength ensures toughness for machine boxes, printer casings, or outdoor use, even in freezing conditions. With heat resistance and low mold shrinkage, PA-763 stays stable in heat-prone applications like coffee machines or displays while ensuring precise, easy molding.

  • Application: for electronics like power panels, TV frames, and car audio consoles
  • Character: Light-resistance, heat-resistance, high-impact, 1.5mm V-0, 2.5mm 5VA
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Strong Flame Resistance

PA-763 ABS meets 1.5mm V-0 and 2.5mm 5VA fire safety standards (UL-94). It keeps electronics like power outlets or TV frames safe from flames.

Tough Against Impacts

High Izod impact strength (22 KJ/m²) resists cracks in car batteries or printer casings. Works well even in freezing temperatures.

Handles Heat & Weather

Stays stable up to 103°C (Vicat), ideal for coffee machines or outdoor displays. Resists sun, heat, and wear over time.

Chimei Polylac® PA-763

Download

Access essential product documentation including technical data sheets, safety information, environmental certifications, and processing guides. All documents are sourced directly from manufacturers and updated regularly for accuracy.

Chimei Polylac® PA-763 Application

Polylac® PA-763 Datasheet

Flame Retardant ABS POLYLAC® PA-763
Product Description: F.R.High heat,Weather resistant
PropertiesISO Test MethodTest ConditionUnitPA-763
Melt Flow Index1133220℃×10KGml/10 min25
Mass Density118323  ℃g/cm31.19
Tensile Strength52750 mm/min, yieldMPa38
50 mm/min, breakMPa29
Tensile Elongation52750 mm/min%20
Flexural Strength1782 mm/minMPa58
Flexural Modulus1782 mm/minGPa2
Izod Impact Strength180/1A23℃, NotchedKJ/m222
-30℃, NotchedKJ/m211
Charpy Impact Strength17923℃, NotchedKJ/m223
-30℃, NotchedKJ/m212
Vicat Softening Temp.30650℃/hr;1KG103
50℃/hr;5KG96
Heat Distortion Temp.75/A1.8MPa, unannealed86
1.8MPa, annealed96
Coefficient of Linear Thermal Expansion113598.5 x 10-5
FlammabilityUL-941.5mm V-0
2.5mm 5VA
Mold Shrinkage294-4%0.3~0.6
Symbol1043>ABS-FR(17)<

Polylac® PA-763 UL Product iQ

POLYLAC® PA-763 UL Product iQ
File Number: E56070Yellow Card™Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLV-0
2.5 mm, Color: ALL5VA
V-0
3.0 mm, Color: ALL5VA
V-0
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLV-0
2.5 mm, Color: ALLV-0
3.0 mm, Color: ALLV-0
FlammabilityIEC 60695-11-20
2.5 mm, Color: ALL5VA
3.0 mm, Color: ALL5VA
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.5 mmPLC 4
2.5 mmPLC 3
High Amp Arc Ignition (HAI)UL 746A
1.5 mmPLC 1
2.5 mmPLC 1
Comparative Tracking Index (CTI)PLC 1UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 3
High Voltage, Low Current Arc ResistancePLC 7
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm60   °C
2.5 mm60   °C
3.0 mm60   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm60   °C
2.5 mm60   °C
3.0 mm60   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm60   °C
2.5 mm60   °C
3.0 mm60   °C
MECHANICAL PROPERTIESVALUETEST METHOD
Tensile Strength39.7   MPaISO 527-2
IMPACT PROPERTIESVALUETEST METHOD
Charpy Impact19   kJ/m²ISO 179-1

Related Polylac® ABS Plastics

No post found!

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top