Chimei Polylac® PA-764 ABS

Chimei Polylac ABS Resin PA-764

Polylac® PA-764 Flame Weather Resistant Grade ABS Resin

Polylac PA-764 ABS Resin by CHIMEI is a flame-retardant, weather-resistant plastic for safe, durable products. It meets strict fire safety standards, perfect for electronics, car batteries, or power panels. With heat resistance up to 101°C and high impact strength (13 KJ/m²), it stays tough in heat or outdoor conditions. Flows smoothly for easy molding of thin parts like TV frames, printer casings, or coffee machines.

  • Character: Light resistance, heat resistance, 1.5mm V-0, 1.5mm 5VB, 2.5mm 5VA
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Superior Flame Retardant Protection

Polylac PA-764 meets strict 1.5mm V-0, 5VB, and 2.5mm 5VA fire safety standards. It stops flames quickly, ideal for electronics, power outlets, and car battery housings needing reliable safety.

High Heat & Impact Resistance

Withstands heat up to 101°C and offers 13 KJ/m² impact strength. Perfect for outdoor gear, coffee machines, or car parts that face tough conditions without cracking.

Easy Molding, Precise Results

Smooth flow (28 ml/10 min) and low shrinkage (0.3–0.6%) ensure easy shaping of thin, complex parts like TV frames or printer casings.

Chimei-Polylac®-PA-764

Download

Access essential product documentation including technical data sheets, safety information, environmental certifications, and processing guides.
All documents are sourced directly from manufacturers and updated regularly for accuracy.

Chimei Polylac® PA-764 Application

Polylac® PA-764 Datasheet

Flame Retardant ABS POLYLAC® PA-764
Product Description: F.R. Weather resistant
PropertiesISO Test MethodTest ConditionUnitPA-764
Melt Flow Index1133220℃×10KGml/10 min28
Mass Density118323  ℃g/cm31.19
Tensile Strength52750 mm/min, yieldMPa36
50 mm/min, breakMPa27
Tensile Elongation52750 mm/min%15
Flexural Strength1782 mm/minMPa55
Flexural Modulus1782 mm/minGPa1.7
Izod Impact Strength180/1A23℃, NotchedKJ/m213
-30℃, NotchedKJ/m27
Charpy Impact Strength17923℃, NotchedKJ/m213
-30℃, NotchedKJ/m27
Vicat Softening Temp.30650℃/hr;1KG101
50℃/hr;5KG90
Heat Distortion Temp.75/A1.8MPa, unannealed82
1.8MPa, annealed92
Coefficient of Linear Thermal Expansion113598.46 x 10-5
FlammabilityUL-941.5mm V-0
1.5mm 5VB
2.5mm 5VA
Mold Shrinkage294-4%0.3~0.6
Symbol1043>ABS-FR(17)<
March 11, 2024

Polylac® PA-764 UL Product iQ

POLYLAC® PA-764(+) UL Product iQ
File Number: E56070Yellow Card™Acrylonitrile Butadiene Styrene (ABS) “POLYLAC”, furnished as pellets
(+) – Indicate 0~0.5% acid scavengers.
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALL5VB
V-0
2.5 mm, Color: ALL5VA
V-0
3.0 mm, Color: ALL5VA
V-0
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLV-0
2.5 mm, Color: ALLV-0
3.0 mm, Color: ALLV-0
FlammabilityIEC 60695-11-20
1.5 mm, Color: ALL5VB
2.5 mm, Color: ALL5VA
3.0 mm, Color: ALL5VA
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.5 mmPLC 1
2.5 mmPLC 1
3.0 mmPLC 0
High Amp Arc Ignition (HAI)UL 746A
1.5 mmPLC 0
2.5 mmPLC 0
3.0 mmPLC 0
Comparative Tracking Index (CTI)PLC 2UL 746A
High Voltage Arc Tracking Rate (HVTR)PLC 2
High Voltage, Low Current Arc ResistancePLC 7
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm75   °C
2.5 mm75   °C
3.0 mm85   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm85   °C
2.5 mm85   °C
3.0 mm85   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm75   °C
2.5 mm75   °C
3.0 mm85   °C

Related Polylac® ABS Plastics

No post found!

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top