Chimei WONDERLOY® PC-860

Chimei WONDERLOY PC-860 PC ASA

WONDERLOY® PC-860 General Purpose Grade UV Stabilized


WONDERLOY PC-860 is a high-performance PC/ASA plastic alloy engineered for demanding outdoor and automotive applications. Combining UV resistance (UL 746C f1), high flow efficiency (22 ml/10min), and 1.5mm HB flammability rating, this material ensures durability, design flexibility, and compliance with strict safety standards.

  • Character: Weather resistance, High flow, 1.5mm HB
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Melt Flow Index: 22 ml/10min
  • Tensile Strength: 52 MPa
  • Izod Impact (23°C): 50 KJ/m²
  • HDT (1.8MPa): 102°C
  • Flammability: 1.5mm HB
  • UV Rating: UL 746C f1

Weatherproof & UV-Resistant

WONDERLOY PC-860 material excels in outdoor environments, resisting fading, cracking, and degradation from UV exposure and moisture. Ideal for automotive trims, solar panels, and outdoor enclosures.

High Flow for Thin-Wall Molding

With a melt flow index of 22 ml/10min, Chimei PC-860 enables complex, lightweight designs (e.g., automotive grilles, electronic housings) while reducing cycle times and material waste.

Toughness in Extreme Conditions

PC-860 retains 50 KJ/m² impact strength at 23°C and 16 KJ/m² at -30°C, ensuring reliability in cold climates or high-stress scenarios like industrial equipment and connectors.

Chimei WONDERLOY PC-860 PC Alloy

Applications

  • Automotive: Mirror housings, grilles, and trim (resists UV fading and road debris).
  • Outdoor Electronics: Junction boxes, LED lamp holders (weatherproof, UL f1 compliant).
  • Consumer Durables: Garden tools, sports equipment (impact-resistant, lightweight).
  • Industrial: Electrical enclosures, connectors (HB flammability, high flow for precision).
Chimei WONDERLOY PC-860 application

Wonderloy® PC-860 Datasheet

General WONDERLOY®  PC-860
Product Description: UV Stabilized
PropertiesISO Test MethodTest ConditionUnitPC-860
Melt Flow Index1133 260℃×5KGml/10
min
22 
Mass Density1183 23 ℃g/cm31.13 
Tensile Strength527 50 mm/min, yieldMPa52 
50 mm/min, breakMPa52 
Tensile Elongation527 50 mm/min%110 
Flexural Strength178 2 mm/minMPa80 
Flexural Modulus2 mm/minGPa2.2 
Izod Impact Strength180/1A23℃, NotchedKJ/m250 
-30℃, NotchedKJ/m216 
Charpy Impact Strength179 23℃, NotchedKJ/m250 
-30℃, NotchedKJ/m216 
Vicat Softening Temp.306 50℃/hr;1KG126 
50℃/hr;5KG119 
Heat Distortion Temp.75/A1.8MPa, unannealed102 
Coefficient of Linear Thermal Expansion11359 8*10-⁵
FlammabilityUL-941.5mm HB
Mold Shrinkage294-4%0.4~0.6
Symbol1043 >PC+ASA<
November 2, 2023
Notes:These are typical properties only and are not to be construed as specifications. Users should confirm results by their own test.

Wonderloy® PC-860 UL Product iQ

WONDERLOY PC-860(f1) | UL Product iQ
File Number: E56070Yellow Card™Polycarbonate/Acrylonitrile Styrene Acrylate (PC/ASA) “WONDERLOY”, furnished as pellets
(f1) – Suitable for outdoor use with respect to exposure to Ultraviolet Light, Water Exposure and Immersion in accordance with UL 746C.
This product has not been received for testing as part of UL Follow-Up Services in the past four years and cannot currently be distributed as a UL Certified product.
FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityANSI/UL 94
1.5 mm, Color: ALLHB
3.0 mm, Color: ALLHB
ISO/IEC FLAMMABILITY PROPERTIESVALUETEST METHOD
FlammabilityIEC 60695-11-10
1.5 mm, Color: ALLHB75
3.0 mm, Color: ALLHB40
ELECTRICAL PROPERTIESVALUETEST METHOD
Hot-wire Ignition (HWI)UL 746A
1.5 mmPLC 4
3.0 mmPLC 3
High Amp Arc Ignition (HAI)UL 746A
1.5 mmPLC 2
3.0 mmPLC 2
Comparative Tracking Index (CTI)PLC 3UL 746A
Dielectric Strength30   kV/mmASTM D149
High Voltage Arc Tracking Rate (HVTR)PLC 4
Volume Resistivity1.0E+12   ohms·cmASTM D257/IEC 60093
Surface Resistivity1.0E+12   ohms/squareASTM D257/IEC 60093
High Voltage, Low Current Arc ResistancePLC 5
THERMAL PROPERTIESVALUETEST METHOD
Relative Thermal Index – Electrical StrengthUL 746B
1.5 mm50   °C
3.0 mm50   °C
Relative Thermal Index – Mechanical ImpactUL 746B
1.5 mm50   °C
3.0 mm50   °C
Relative Thermal Index – Mechanical StrengthUL 746B
1.5 mm50   °C
3.0 mm50   °C
PHYSICAL PROPERTIESVALUETEST METHOD
UV Exposure & Water Immersionf1UL 746C

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top