TAIRIREX® NX3400
TAIRISAN NX3400 by Formosa Chemicals is a high-performance Styrene Acrylonitrile (SAN) resin. Combining high heat resistance (up to 102°C) and excellent chemical stability, this material is ideal for precision-molded components like fan blades and battery housings. Its low shrinkage and ease of processing ensure consistent quality in industrial settings.
- Manufacturer: FCFC (Formosa Chemicals & Fibre Corporation)
- Character: High heat, Chemical resistance
- Application: Blade of fan, Batteries housing
Key technical data (ISO)
- Melt Flow Index (220°C/10kg): 10 g/10 min (ISO 1133)
- Tensile Strength: 83 MPa (ISO 527)
- Flexural Modulus: 3600 MPa (ISO 178)
- Heat Deflection Temp: 104°C (ISO 75/A)
- Rockwell Hardness: R-79 (ISO 2039-2)
- Flame Rating: UL94 HB (1.6–1.8 mm thickness)
- Molding Shrinkage: 0.4–0.7% (ISO 2577)