Makrolon® 2605 Polycarbonate PC Resin Injection molding Grade
Makrolon 2605 by Covestro is a versatile, medium-viscosity polycarbonate resin ideal for injection molding. With an MVR of 12 cm³/10 min (300°C/1.2 kg), it offers easy processing, excellent release properties, and is available in transparent, translucent, or opaque colors. Perfect for demanding industrial applications.
- Character: MVR (300 °C/1.2 kg) 12 cm³/10 min; general purpose; medium viscosity; easy release; injection molding – melt temperature 280 – 320 °C; available in transparent, translucent and opaque colors
- Application: General purpose grades / Medium viscosity
Key technical data
Mechanical Properties
- Tensile Modulus: 2,400 MPa
- Flexural Strength: 97 MPa
- Strain at Break: >120%
- Notched Impact (23°C): 70 kJ/m² (ISO 179)
Thermal Performance
- HDT @0.45 MPa: 136°C (ISO 75)
- Vicat Softening Temp: 144°C (ISO 306)
- Linear Thermal Expansion: 0.65 x 10⁻⁵/K
Electrical & Safety
- CTI: 250 (IEC 60112)
- UL 94 Rating: V-2 (0.75mm), HB (2.5mm)
- Volume Resistivity: 1E14 Ω·m
Processing (Optimal)
- Melt Temp: 280–320°C
- Mold Temp: 80–120°C
- Drying: 120°C for 2–3 hrs (<0.02% moisture)
Application
- Automotive: Lens housings and dashboard components resisting heat deformation.
- Electronics: Flame-retardant (V-2) power tool casings and EV battery covers.
- Industrial: Impact-resistant safety visors and machine guards.
- Consumer Goods: Durable transparent kitchenware and appliance panels.
- Lighting: High-clarity (89% transmittance) diffusers and LED covers.
Features & Benefits
Related Makrolon® PC Plastics
Covestro Apec® 1897 PC Resin
Covestro Apec® 1895 PC Resin
Covestro Apec® 1803 PC Resin
Covestro Makrolon® 1804 PC Resin
Covestro Makrolon® Rx1805 RE
Covestro Makrolon® 2858 RE
Covestro Makrolon® 2658 RE
Covestro Makrolon® 2458 RE
Covestro Makrolon® 2258 RE
Covestro Makrolon® Rx2530
Covestro Makrolon® Rx1851
Covestro Makrolon® Rx1805
Covestro Makrolon® Rx1452
Covestro Makrolon® 3158 PC Resin
Covestro Makrolon® 2658 PC Resin
Covestro Makrolon® 2558 PC Resin
Covestro Makrolon® 2258 PC Resin
Covestro Makrolon® 6267 X RE CQ
Advanced Manufacturing