Covestro Makrolon® AL2647 PC Resin

Makrolon PC Polycarbonate

Makrolon AL2647 Polycarbonate Granules Injection Molding Grade

Covestro Makrolon AL2647 is a medium-viscosity, UV-stabilized polycarbonate resin engineered for automotive lighting. With an MVR of 12 cm³/10 min (300°C/1.2 kg), it offers easy mold release and comes in crystal-clear or vibrant signal colors—perfect for high-precision injection-molded lenses.

  • Character: MVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; UV stabilized; easy release; available in clear transparent colors and in various signal colors
  • Application: Injection molding; Automotive lighting; Headlamp lenses for automotive forward lighting
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Flow: MVR 12 cm³/10 min (300°C/1.2 kg, ISO 1133)
  • Strength: Tensile modulus 2,400 MPa | Flexural strength 98 MPa (ISO 527/178)
  • Thermal: HDT 123°C (1.8 MPa) | Vicat softening 143°C (ISO 75/306)
  • Optical: 88–89% transmittance (1–3 mm) | Haze <0.5% (ISO 13468-2/14782)
  • Durability: Water absorption 0.12% (50% RH) | UL 94 V-2 rated (0.75 mm)

Application

  • Automotive forward lighting (e.g., headlamp lenses, fog lights)
  • Signal lighting components (brake lights, turn indicators)
  • Thin-wall injection-molded covers requiring optical precision and weather resistance

Features & Benefits

Optical Clarity & UV Stability

Achieve >88% light transmission (ISO 13468-2) and near-zero haze (<0.5%) for distortion-free headlamp lenses, even after years of sun exposure. Ensures compliance with automotive safety standards.

Impact Resistance Under Stress

Withstands 60J puncture energy (ISO 6603-2) and 70 kJ/m² notched impact strength (ISO 179) at 23°C. Prevents lens cracking from road debris or thermal shocks.

Thermal & Processing Efficiency

Maintains integrity at 123°C (1.8 MPa load, ISO 75) and flows smoothly at 280–320°C. Easy-release properties cut cycle times by 15% vs. standard PC resins.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top