Makrolon LED2045 Polycarbonate Granules Optical Grade
Covestro Makrolon LED2045 is an optically clear polycarbonate resin engineered for precision light guides. With high melt flow (17 cm³/10min), exceptional transparency (>90% transmittance), and low viscosity, it enables easy molding of complex optical components while ensuring consistent color purity (available only in crystal-clear 000000 grade).
- Character: MVR (250 °C/2.16 kg) 17 cm³/10 min; PC with highest transmission; low viscosity; easy release;available in color code 000000 only; Transparent, Optical quality
- Application: Injection molding; Light guides
Key technical data
- Refractive Index: 1.594
- Haze (3mm): <0.5%
- Transmittance (1mm): 90%
- Tensile Modulus: 2,350 MPa
- Flexural Strength: 97 MPa
- Notched Impact (23°C): 50 kJ/m²
- HDT (1.8 MPa): 124°C
- Vicat Softening: 145°C
- CTI: 225 (Solution A)
- Melt Temp: 250–300°C
- Mold Temp: 80–120°C
- Drying: 120°C for 2–3 hours
Application
- LED Light Guides: Edge-lit panels, automotive taillights, and backlit displays requiring uniform diffusion.
- Optical Lenses: Thin-walled lenses for sensors and consumer electronics.
- Transparent Housings: Protective covers for indicators and control panels.
- Precision Components: Medical device light pipes and touch-screen interfaces.
Features & Benefits
Related Makrolon® PC Plastics
Covestro Apec® 1897 PC Resin
Covestro Apec® 1895 PC Resin
Covestro Apec® 1803 PC Resin
Covestro Makrolon® 1804 PC Resin
Covestro Makrolon® Rx1805 RE
Covestro Makrolon® 2858 RE
Covestro Makrolon® 2658 RE
Covestro Makrolon® 2458 RE
Covestro Makrolon® 2258 RE
Covestro Makrolon® Rx2530
Covestro Makrolon® Rx1851
Covestro Makrolon® Rx1805
Covestro Makrolon® Rx1452
Covestro Makrolon® 3158 PC Resin
Covestro Makrolon® 2658 PC Resin
Covestro Makrolon® 2558 PC Resin
Covestro Makrolon® 2258 PC Resin
Covestro Makrolon® 6267 X RE CQ
Advanced Manufacturing