Covestro Makrolon® 2807 RE

Makrolon PC Polycarbonate

Makrolon 2807 RE Polycarbonate Granules Genaral Injection Molding Grade

Makrolon® 2807 RE is a versatile, medium-viscosity polycarbonate resin designed for injection molding. Featuring UV stabilization, easy mold release, and transparency, it combines performance with sustainability via bio-circular ISCC PLUS mass balance. Ideal for demanding applications requiring clarity and durability.

  • Character: MVR (300 °C/1.2 kg) 9.0 cm³/10 min; medium viscosity; UV stabilized; easy release; available in transparent, translucent and opaque colors. CQ renewable attributed
  • Application: Injection molding; General purpose
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Flow Rate (MVR): 9.0 cm³/10 min (300°C/1.2 kg)
  • Tensile Modulus: 2,400 MPa
  • Flexural Strength: 98 MPa
  • Ball Indentation Hardness: 115 N/mm²
  • Heat Deflection (1.8 MPa): 124°C
  • Thermal Expansion: 0.65 x 10⁻⁵/K
  • CTI: 250 (Solution A)
  • Electrical Strength: 34 kV/mm
  • Luminous Transmittance: 89% (1 mm thickness)
  • Haze: <0.8%

Application

  • Consumer Electronics: Transparent phone cases, charger housings.
  • Automotive Parts: Interior trim, light covers, and dash components.
  • Industrial Equipment: Protective covers, machine guards, and enclosures.
  • Lighting Solutions: LED diffusers and outdoor fixture lenses.

Features & Benefits

Sustainable Bio-Circular Material

Derived partially from renewable resources (ISCC PLUS-certified), Makrolon 2807 RE reduces carbon footprint without sacrificing performance. Perfect for eco-conscious manufacturing.

Exceptional Impact Resistance

With Charpy notched impact strength of 75 kJ/m² (23°C), it withstands heavy shocks and drops. Ensures product longevity in rugged environments.

Reliable Thermal Stability

Vicat softening at 143°C and UL 94 V-2 flame rating (0.75 mm) ensures safety in high-heat applications like electronics and automotive components.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top