Covestro Makrolon® AG2677 RE

Makrolon PC Polycarbonate

Makrolon AG2677 RE Polycarbonate Granules

Makrolon® AG2677 RE is a medium-viscosity polycarbonate resin with UV stabilization and easy-release properties. Featuring 12 cm³/10 min MVR flow and optical-grade transparency, it integrates renewable content via ISCC PLUS mass balance—ideal for sustainable, high-clarity injection-molded parts.

  • Character: MVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; UV stabilized; easy release; available in transparent colors only. CQ renewable attributed, Optical quality
  • Application: Injection molding; General purpose
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Flow Rate: 12 cm³/10 min (300°C/1.2 kg)
  • HDT @1.8 MPa: 124°C
  • Vicat Softening: 143°C
  • Tensile Modulus: 2,400 MPa
  • Notched Impact (23°C): 70 kJ/m²
  • CTI: 250
  • Volume Resistivity: 1E14 Ω·m
  • Transmittance (3mm): 88%
  • Haze: <0.8%

Application

  • Consumer Electronics: Phone cases, transparent covers.
  • Automotive: Interior trim, light diffusers.
  • Industrial: Safety visors, meter housings.
  • Renewable-Focused Packaging: Premium transparent containers.
  • General Purpose: Replacements for glass or standard plastics.

Features & Benefits

Sustainable Material Sourcing

Partially bio-circular via ISCC PLUS mass balance, reducing carbon footprint while maintaining performance. Perfect for eco-driven brands targeting greener certifications.

Optical Clarity & UV Resistance

It delivers 88–89% luminous transmittance and <0.8% haze (3mm thickness) with built-in UV stabilization. Ensures long-term visual appeal for outdoor or display applications.

Easy Processing & Durability

Medium flow (12 cm³/10 min MVR) and easy-release properties streamline injection molding. Withstands 124°C heat deflection and 70 kJ/m² impact strength for rugged use.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top