Makrolon LED2245 EL Polycarbonate Granules
Makrolon LED2245 EL is a low-viscosity, easy-release polycarbonate resin optimized for injection molding. With an MVR of 34 cm³/10 min (300°C/1.2 kg) and exceptional optical clarity (>85% transmittance), it streamlines production of precision light guides and optical components.
- Character: flame retardant; MVR (300 °C/1.2 kg) 5.0 cm³/10 min; low diffusion; UV stabilized. Transparent, Optical quality.
- Application: Extrusion; Injection molding; Light diffusion
Key technical data (ISO)
- MVR: 34 cm³/10 min (300°C/1.2 kg)
- Shrinkage: 0.69% (parallel), 0.70% (normal)
- Transmittance: >85% (4mm thickness)
- Haze: <13%
- Impact Strength (Charpy, 23°C): 60 kJ/m²
- Puncture Energy: 50 J (23°C)
- HDT: 125°C (1.8 MPa), 138°C (0.45 MPa)
- Continuous Use: Up to 120°C
- Melt Temp: 250–300°C
- Mold Temp: 80–120°C
- Drying: 120°C for 2–3 hours
Application
- LED Light Guides: Edge-lit panels for TVs, monitors, and automotive dashboards.
- Optical Components: Lenses, diffusers, and light pipes in consumer electronics.
- Signage & Displays: Backlit advertising panels and touchscreen interfaces.
- Architectural Lighting: Slim-profile LED fixtures requiring uniform illumination.
Features & Benefits
Related Makrolon® PC Plastics
Covestro Apec® 1897 PC Resin
Covestro Apec® 1895 PC Resin
Covestro Apec® 1803 PC Resin
Covestro Makrolon® 1804 PC Resin
Covestro Makrolon® Rx1805 RE
Covestro Makrolon® 2858 RE
Covestro Makrolon® 2658 RE
Covestro Makrolon® 2458 RE
Covestro Makrolon® 2258 RE
Covestro Makrolon® Rx2530
Covestro Makrolon® Rx1851
Covestro Makrolon® Rx1805
Covestro Makrolon® Rx1452
Covestro Makrolon® 3158 PC Resin
Covestro Makrolon® 2658 PC Resin
Covestro Makrolon® 2558 PC Resin
Covestro Makrolon® 2258 PC Resin
Covestro Makrolon® 6267 X RE CQ
Advanced Manufacturing