Covestro Makrolon® 9125 PC resin

Makrolon PC Polycarbonate

Makrolon 9125 PC Resin

Covestro Makrolon 9125 is a 20% glass fiber-reinforced, flame-retardant PC-GF20 resin (ISO: PC-GF20 FR). With medium viscosity and easy mold release, it delivers dimensional stability (0.3–0.5% shrinkage), UL 94V-0 compliance at 1.5mm, and MVR of 8.0 cm³/10 min (300°C/1.2 kg). Ideal for injection-molded opaque industrial parts.

  • Character: 20 % glass fiber reinforced; flame retardant; MVR (300 °C/1.2 kg) 8.0 cm³/10 min; UL 94V-0/1.5 mm; medium viscosity; easy release; available in opaque colors only; Dimensionally stable.
  • Application: Injection molding
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Tensile Strength: 85 MPa
  • Flexural Modulus: 5,600 MPa
  • Charpy Notched Impact: 8 kJ/m² (23°C)
  • Ball Indentation Hardness: 148 N/mm²
  • HDT (1.8 MPa): 138°C
  • CTI: 175
  • Volume Resistivity: 1 × 10¹⁴ Ω·m (IEC 62631)
  • Thermal Conductivity: 0.23 W/(m·K)
  • Melt Temp: 280–320°C (standard: 300°C)
  • Mold Temp: 80–120°C
  • Density: 1,340 kg/m³
  • Water Absorption: 0.10% (23°C/50% RH)

Application

  • Electrical: Connector housings, circuit breakers (UL V-0 compliant).
  • Automotive: Sensor mounts, ignition components (heat resistant).
  • Industrial: Power tool casings, enclosure panels (high stiffness).
  • Consumer: Appliance housings, safety goggles (impact resistant).

Features & Benefits

Superior Flame Resistance

Makrolon 9125 achieves UL 94V-0 (1.5mm), V-2 (0.36mm), and 35% oxygen index. It eliminates fire risks in electrical/electronic components without secondary coatings.

Reinforced Mechanical Strength

20% glass fiber boosts tensile strength (85 MPa) and stiffness (5,800 MPa modulus). Ensures structural integrity in load-bearing parts like automotive brackets.

High Thermal Stability

It withstands 138°C at 1.8 MPa (HDT) and 145°C Vicat softening. Maintains performance in high-heat environments like power tools or LED housings.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity

Scroll to Top