Covestro Makrolon® 2856 RE CQ

Makrolon PC Polycarbonate

Makrolon 2856 RE CQ PC Resin Partially Bio-circular Grade

Makrolon® 2856 RE CQ is a medium-viscosity, food-contact-compliant polycarbonate resin with renewable content (CQ attribution). Featuring easy release and an MVR of 9.0 cm³/10 min (300°C/1.2 kg), it’s optimized for injection molding (280–320°C melt temp) and available in transparent/opaque colors.

  • Character: food contact quality; medium viscosity; easy release; injection molding – melt temperature 280 – 320 °C; available in transparent, translucent and opaque colors; CQ renewable attributed
  • Application: Injection molding
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data (ISO)

  • Flow Rate: 9.0 cm³/10 min (300°C/1.2 kg)
  • Strength: Tensile modulus 2,400 MPa; yield stress 65 MPa
  • Impact: Charpy notched 75 kJ/m² (23°C); puncture energy 60 J
  • Thermal: HDT 125°C (1.8 MPa); Vicat softening 145°C
  • Safety: UL 94 V-2 (0.75 mm), HB (2.5 mm); CTI 250 (electrical safety)
  • Clarity: 88% light transmission (3 mm thickness)
  • Stability: Low water absorption (0.12% equilibrium)
  • Compliance: ISCC PLUS, FDA-compliant for food contact

Application

  • Food Packaging: Containers, lids, and beverage tumblers
  • Consumer Goods: Power tool housings, appliance components
  • Electrical: Connectors, switches
  • Automotive: Interior trim, light covers
  • Medical: Non-implant device housings

Features & Benefits

Renewable & Sustainable Sourcing

Partially bio-circular via ISCC PLUS mass balance, reducing carbon footprint while maintaining performance. Ideal for brands targeting eco-friendly manufacturing without compromising quality.

Superior Impact & Heat Resistance

It withstands 75 kJ/m² notched impact (23°C) and 125°C heat deflection (1.8 MPa). Perfect for durable products like power tool housings or automotive parts exposed to stress.

Food-Safe & Versatile Processing

Food-contact compliant and easy to mold (low shrinkage: 0.6–0.8%). Simplifies production of kitchenware, packaging, and medical components needing clarity and safety.

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top