Makrolon 3158 PC Resin
Makrolon 3158 is a high-viscosity, biocompatible polycarbonate resin engineered for demanding medical applications. With an MVR of 6.0 cm³/10 min (300°C/1.2 kg), it offers easy mold release, exceptional clarity (88% transmittance at 3mm), and compliance with ISO 10993-1 biocompatibility standards. Ideal for sterilization-critical devices.
- Character: MVR (300 °C/1.2 kg) 6.0 cm³/10 min; high viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colors
- Application: Injection molding; Medical devices; Suitable for ETO and steam sterilization at 121 °C
Key technical data (ISO)
- Tensile Strength: 70 MPa | Flexural Modulus: 2,400 MPa
- Notched Impact (23°C): 80 kJ/m² (non-break) | Puncture Force: 6,500 N
- Heat Deflection (1.8 MPa): 126°C | Glass Transition: 146°C
- Linear Expansion: 0.65 x 10⁻⁴/K (minimizes warpage)
- Luminous Transmittance: 89% (1mm)
- Haze: <0.8% (crystal-clear lenses)
- Processing Melt Temp: 290–330°C
- Processing Mold Temp: 80–100°C
- Processing Drying: 120°C/2–3 hrs
Download
Application
- Sterilizable medical devices: Surgical instrument housings, dialysis components.
- Injection-molded labware: Petri dishes, transparent fluid reservoirs.
- ETO/steam-sterilized (121°C) equipment: IV drip chambers, respirator valves.
Features & Benefits
Related Makrolon® PC Plastics
Covestro Apec® 1897 PC Resin
Covestro Apec® 1895 PC Resin
Covestro Apec® 1803 PC Resin
Covestro Makrolon® 1804 PC Resin
Covestro Makrolon® Rx1805 RE
Covestro Makrolon® 2858 RE
Covestro Makrolon® 2658 RE
Covestro Makrolon® 2458 RE
Covestro Makrolon® 2258 RE
Covestro Makrolon® Rx2530
Covestro Makrolon® Rx1851
Covestro Makrolon® Rx1805
Covestro Makrolon® Rx1452
Covestro Makrolon® 3158 PC Resin
Covestro Makrolon® 2658 PC Resin
Covestro Makrolon® 2558 PC Resin
Covestro Makrolon® 2258 PC Resin
Covestro Makrolon® 6267 X RE CQ
Advanced Manufacturing