Makrolon Rx2530 PC Resin Medical Devices
Makrolon Rx2530 by Covestro is a medical-grade polycarbonate resin engineered for critical healthcare applications. With medium viscosity (MVR 15 cm³/10 min) and ISO 10993-1 biocompatibility, it delivers exceptional clarity, radiation sterilization resilience, and reliability for transparent medical components.
- Character: MVR (300 °C/1.2 kg) 15 cm³/10 min; medium viscosity; suitable for sterilization with high-energy radiation; biocompatible.
- Application: Injection molding; Medical devices; Transparent parts for medical devices.
Key technical data (ISO)
- Tensile Modulus: 2,400 MPa
- Puncture Impact Energy: 60 J (23°C)
- Heat Deflection (1.8 MPa): 134°C
- Glass Transition Temp: 142°C
- Water Absorption: 0.30% saturation
- Oxygen Index: 27% – Flame-retardant
- Melt Temp: 280–320°C
- Drying: 120°C for 2–3 hours
Application
- Medical Devices: Surgical instrument housings, dialysis components.
- Transparent Medical Parts: IV connectors, blood reservoirs, diagnostic cartridges.
- Injection-Molded Sterilizable Items: Autoclavable trays, implant packaging.
Features & Benefits
Related Makrolon® PC Plastics
Covestro Apec® 1897 PC Resin
Covestro Apec® 1895 PC Resin
Covestro Apec® 1803 PC Resin
Covestro Makrolon® 1804 PC Resin
Covestro Makrolon® Rx1805 RE
Covestro Makrolon® 2858 RE
Covestro Makrolon® 2658 RE
Covestro Makrolon® 2458 RE
Covestro Makrolon® 2258 RE
Covestro Makrolon® Rx2530
Covestro Makrolon® Rx1851
Covestro Makrolon® Rx1805
Covestro Makrolon® Rx1452
Covestro Makrolon® 3158 PC Resin
Covestro Makrolon® 2658 PC Resin
Covestro Makrolon® 2558 PC Resin
Covestro Makrolon® 2258 PC Resin
Covestro Makrolon® 6267 X RE CQ
Advanced Manufacturing