CYCOLOY™ FR Resins CM6220

Sabic CYCOLOY™ FR Resins

Sabic Cycoloy FR CM6220 (PC/ABS) Resin

Cycoloy Fr resins CM6220 is a mineral filled modified PC blend featuring of high modulus (6GPa), good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall flame resistance and various environmental requirements.

  • Character:
  • Application:
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data

  • Flame Rating (UL 94): V-0 @ 1.5 mm | 5VB @ 1.5 mm
  • Tensile Strength at Yield: 55 MPa
  • Flexural Modulus: 6030 MPa
  • Izod Impact, Notched (ASTM D256, 23°C): 95 J/m
  • Heat Deflection Temp (HDT, 1.82 MPa): 85 °C
  • Melt Flow Rate (260°C/2.16 kg): 12 g/10 min
  • Specific Gravity: 1.39

Application

  • Electrical Enclosures and Housings
  • Connectors and Sockets
  • Consumer Electronics Components
  • Thin-Wall Appliances and Parts

Features & Benefits

Superior Non-Halogen Flame Retardancy

CM6220 achieves UL94 V-0 (1.5mm) without bromine or chlorine, meeting strict safety and environmental standards for electronics and enclosures.

High Stiffness with Exceptional Flow

Its high modulus (6 GPa) and good melt flow ensure easy filling of complex, thin-walled parts, reducing warpage and enabling lighter, stronger designs.

Robust Mechanical & Impact Performance

The material maintains a good balance of ductility and impact strength, helping your components withstand assembly stresses and minor impacts during use.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top