CYCOLOY™ FR Resins CY6310

Sabic CYCOLOY™ FR Resins

Sabic Cycoloy FR CY6310 (PC/ABS) Resin

Cycoloy Fr resins CY6310 is a high-flow, flame-retardant PC/ABS blend. It offers exceptional impact strength and heat resistance, making it ideal for large, thin-walled components requiring UL94 V-0 and 5VA ratings without halogenated flame retardants.

  • Character:
  • Application:
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data

  • Tensile Strength (Yield): 63 MPa
  • Flexural Modulus: 2700 MPa
  • Izod Impact (Notched, 23°C): 600 J/m
  • Thermal HDT @ 1.82 MPa: 90 °C
  • Vicat Softening Temperature (B/50): 109 °C
  • UL94 Rating: V-0 @ 1.5 mm | 5VA @ 2.9 mm
  • Glow Wire Flammability Index (GWFI): 960 °C @ 3.0 mm
  • Melt Flow Rate (260°C/2.16 kg): 20 g/10 min
  • Specific Gravity: 1.17

Application

  • Electric Vehicle (EV) Battery Components
  • Large Consumer Electronics Housings (e.g., Printers, Monitors)
  • Power Distribution Units (PDUs) and Electrical Enclosures
  • Industrial Control Systems and Housings
  • Telecommunications Infrastructure Equipment

Features & Benefits

Flame Retardancy Without Halogens

This non-chlorinated/brominated grade achieves a UL94 V-0 rating at 1.5mm, ensuring superior fire safety for electronics and enabling compliance with stringent environmental regulations.

Exceptional Impact Strength & Durability

With high notched Izod impact resistance, Cycoloy CY6310 resin withstands physical shocks and stresses, resulting in durable end-products that reduce the risk of failure in demanding applications.

High Flow for Complex & Large Parts

The high melt flow rate ensures easy filling of intricate molds and large-sized parts, leading to excellent surface finishes, reduced injection pressure, and higher production efficiency.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity