Key technical data

  • Tensile Stress at Yield: 64 MPa (ASTM D638)
  • Tensile Modulus: 2330 MPa (ASTM D638)
  • Izod Impact, Notched (+23°C): 15 kJ/m²
  • Heat Deflection Temp (HDT) @ 1.82 MPa: 118 °C
  • Vicat Softening Temperature: 133 °C
  • Relative Temperature Index (Electrical): 105 °C
  • Ball Pressure Test (125°C): Pass
  • Comparative Tracking Index (CTI): 175 V
  • Volume Resistivity: 1.E+15 Ω·cm
  • UL 94 Rating: V-0 @ 1.2 mm | 5VB @ 2.5 mm
  • Glow Wire Ignitability (GWI): 775 °C
  • Oxygen Index (LOI): 32%
  • Melt Volume Rate (260°C/5.0 kg): 13 cm³/10 min
  • Mold Shrinkage: 0.4 – 0.8 %
  • Density: 1.20 g/cm³

Application

  • Electrical Enclosures and Housings
  • Power Distribution Units (PDUs)
  • Circuit Breakers and Switches
  • Connectors and Sockets
  • Automotive Electrical Components
  • Charging Stations and EV Components
  • Consumer Electronics Housings

Features & Benefits

Flame Retardancy Without Halogens

This non-chlorinated/brominated grade achieves UL94 V-0 at 1.2mm, ensuring critical fire safety for thinner, lighter designs while meeting stringent environmental standards.

Exceptional Impact Strength & Durability

Its high impact resistance, even at -30°C, means your components can withstand accidental drops, assembly stress, and harsh operating conditions without cracking.

High Heat Resistance

With a Heat Deflection Temperature of 118°C, Cycoloy CY6414 resin maintains structural integrity in high-temperature settings, such as near heat-generating electronic parts.

Sabic Cycoloy FR Resins particles

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top