Valox FR PBT 357U Flame Retardant Grade
Valox FR PBT 357U is a flame-retardant, impact-modified thermoplastic. It offers superior chemical resistance and achieves a UL94 V-0 rating at just 0.64mm, making it an ideal, safe choice for demanding electrical components.
- Character: unreinforced, UV stabilized, impact modified flame retardant
Key technical data
- Flame Rating: UL 94 V-0 @ 0.64 mm | 5VA @ 3.0 mm
- Heat Resistance: HDT @ 1.82 MPa: 98°C
- Tensile Strength (Yield): 48 MPa
- Flexural Modulus: 2060 MPa
- Notched Izod Impact: 534 J/m
- Volume Resistivity: >1.2E+16 Ω·cm
- Dielectric Strength: 18.5 kV/mm
- Specific Gravity: 1.34
- Water Absorption: 0.08% (24hrs)
- Melt Temperature: 250 – 265 °C
- Mold Temperature: 50 – 75 °C
- Drying: 3-4 hours at 120°C
Application
- Bobbins and Coil Formers
- Circuit Breakers and Switches
- Electrical Connectors and Enclosures
- Other Critical Electrical Insulation Components
Features & Benefits

Related Valox™ FR PBT Products
VALOX™ FR PBT V4860HR
VALOX™ FR PBT V4760
VALOX™ FR PBT V3900WX
VALOX™ FR PBT V3504
VALOX™ FR PBT SHF3800UX
VALOX™ FR PBT DR48
VALOX™ FR PBT 4631
VALOX™ FR PBT 4521
VALOX™ FR PBT 4512
VALOX™ FR PBT 3706
VALOX™ FR PBT 865
VALOX™ FR PBT 771
VALOX™ FR PBT 855
VALOX™ FR PBT 855
VALOX™ FR PBT 780
VALOX™ FR PBT 553U
VALOX™ FR PBT 457
VALOX™ FR PBT 420SE0
Advanced Manufacturing