Valox FR PBT 357XU Flame Retardant Grade
VALOX™ FR Resin 357XU is a flame-retardant, impact-modified PC/PBT blend. It offers superior chemical resistance and achieves top UL94 V-0 and 5VA ratings in thin walls, making it ideal for demanding electrical and electronic components.
- Character: unreinforced, UV stabilized, impact modified flame retardant, excellent chemical resistance
Key technical data
- Flame Ratings: UL94 V-0 @ 0.75mm, 5VA @ 2.5mm
- Relative Temperature Index (RTI): 120°C
- Tensile Strength at Yield: 50 MPa
- Tensile Modulus: 2100 MPa
- Notched Izod Impact (23°C): 40 kJ/m²
- Heat Deflection Temp (HDT) @ 1.82 MPa: 85°C
- Specific Gravity / Density: 1.34
- Mold Shrinkage (Flow): 1.1 – 1.8%
- Comparative Tracking Index (CTI): 200 V (IEC 60112)
Application
- Electrical Bobbins and Coil Formers
- Circuit Breakers and Switches
- Electrical Enclosures and Housings
- Connectors and Sockets
- Automotive Electrical Components
Features & Benefits

Related Valox™ FR PBT Products
VALOX™ FR PBT V4860HR
VALOX™ FR PBT V4760
VALOX™ FR PBT V3900WX
VALOX™ FR PBT V3504
VALOX™ FR PBT SHF3800UX
VALOX™ FR PBT DR48
VALOX™ FR PBT 4631
VALOX™ FR PBT 4521
VALOX™ FR PBT 4512
VALOX™ FR PBT 3706
VALOX™ FR PBT 865
VALOX™ FR PBT 771
VALOX™ FR PBT 855
VALOX™ FR PBT 855
VALOX™ FR PBT 780
VALOX™ FR PBT 553U
VALOX™ FR PBT 457
VALOX™ FR PBT 420SE0
Advanced Manufacturing