Valox FR PBT 362 Flame Retardant Grade
VALOX™ FR Resin 362 is a flame-retardant, unreinforced PBT plastic resin. It offers superior electrical properties and a UL94 V-0 rating, making it ideal for critical electrical components like relay sockets and switches.
- Character: Unreinforced PBTP, UL94 V-0 rated. Non-blooming flame retardant. Excellent electrical properties. High tracking index.
Key technical data
- Flame Rating: UL 94 V-0 @ 1.5 mm
- Relative Temperature Index (RTI): 75°C
- HDT: 120°C @ 0.45 MPa / 50°C @ 1.8 MPa
- Tensile Strength at Yield: 45 MPa
- Impact Strength (Izod Notched): 5 kJ/m²
- Comparative Tracking Index (CTI): 600 V
- Dielectric Strength: 28 kV/mm (at 0.8mm)
- Mold Shrinkage: 1.1 – 1.8% (Flow)
- Melt Temperature: 250 – 270°C
Download
Application
- Relay Sockets
- Switches
- Electrical Connectors
- Circuit Breaker Components
- Other Critical Electrical Insulation Parts
Features & Benefits

Related Valox™ FR PBT Products