Valox FR PBT 364 Flame Retardant Grade
VALOX™ FR PBT 364 is a flame-retardant PBT plastic, offering superior impact strength and chemical resistance. It is UL94 V-0 rated at 1.47mm, making it an ideal, reliable choice for demanding outdoor telecom enclosures.
- Character: unreinforced, impact modified flame retardant
Key technical data
- Flame Rating: UL 94 V-0 @ 1.47 mm / 5VA @ 3.0 mm
- HDT @ 1.82 MPa: 68°C
- Vicat Softening Point (B/50): 115°C
- Tensile Strength at Break: 36 MPa
- Flexural Modulus: 1800 MPa
- Notched Izod Impact (23°C): 747 J/m
- Specific Gravity: 1.3
- Mold Shrinkage: 0.8 – 1.0%
- Melt Flow Rate (266°C/5kg): 19 g/10 min
- Melt Temperature: 250 – 265°C
- Mold Temperature: 50 – 75°C
- Drying: 3-4 hours at 120°C
Application
- Outdoor Telecommunications Enclosures
Features & Benefits

Related Valox™ FR PBT Products