Valox FR PBT 553U Flame Retardant Grade
VALOX™ FR resin 553U is a 30% glass-filled, flame-retardant PBT/PC blend. It offers superior strength, minimal warpage, and a UL94 V-0 rating at 0.86mm, ideal for demanding electrical and structural components.
- Character: 30% glass filled, UV stabilized flame retardant
Key technical data
- Flame Rating: UL 94 V-0 @ 0.86 mm / 5VA @ 2.31 mm
- Heat Resistance (HDT): 160°C @ 1.82 MPa
- Tensile Strength (Break): 110 MPa
- Flexural Modulus: 9400 MPa
- Impact Strength (Notched Izod): 85 J/m
- Relative Temperature Index (Elec.): 125°C
- Specific Gravity: 1.58
- Mold Shrinkage (Flow): 0.3 – 0.5%
Application
- Appliance Handles
- Spotlights & Lighting Housings
- Electric Motor Components
- Pump Housings
Features & Benefits

Related Valox™ FR PBT Products
VALOX™ FR PBT V4860HR
VALOX™ FR PBT V4760
VALOX™ FR PBT V3900WX
VALOX™ FR PBT V3504
VALOX™ FR PBT SHF3800UX
VALOX™ FR PBT DR48
VALOX™ FR PBT 4631
VALOX™ FR PBT 4521
VALOX™ FR PBT 4512
VALOX™ FR PBT 3706
VALOX™ FR PBT 865
VALOX™ FR PBT 771
VALOX™ FR PBT 855
VALOX™ FR PBT 855
VALOX™ FR PBT 780
VALOX™ FR PBT 553U
VALOX™ FR PBT 457
VALOX™ FR PBT 420SE0
Advanced Manufacturing