VALOX™ FR resin 771 is a 35% mineral/glass-filled, flame-retardant PBT grade. It offers superior chemical resistance, a UL94 V-0 rating at 0.75mm, and exceptional protection against electrical arcing, making it ideal for demanding electrical components.

  • Character: 35% mineral/glass filled, flame retardant
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Tensile Strength (Break): 72 MPa
  • Flexural Modulus: 5860 MPa
  • Notched Izod Impact (23°C): 42 J/m
  • Heat Deflection Temperature (HDT @ 1.82 MPa): 196°C
  • Relative Temp Index (Electrical): 140°C
  • Relative Temp Index (Mechanical w/ Impact): 125°C
  • Ball Pressure Test (175°C): Passes
  • Comparative Tracking Index (CTI): 600 V (PLC 0)
  • Arc Resistance: 4 (RLC Code)
  • Volume Resistivity: >1E+15 Ω·cm
  • UL 94 Flame Class Rating: V-0 @ 0.75 mm, 5VA @ 2.0 mm
  • Glow Wire Ignitability (3.0mm): 800°C
  • Specific Gravity: 1.7
  • Mold Shrinkage (Flow): 0.65 – 0.85%

Application

  • Circuit Breakers and Switches
  • Electrical Connectors
  • Motor Housings and Commutators
  • Power Distribution Components
  • Automotive Electrical Systems
  • Appliance Controllers and Relays

Features & Benefits

Superior Flame Retardant Performance

VALOX 771 achieves a UL94 V-0 rating at just 0.75mm, ensuring critical safety in thin-walled components. This allows for design flexibility without compromising on fire safety in enclosures and connectors.

Exceptional Electrical Safety

With a CTI of 0 and high arc resistance, VALOX™ FR resin 771 withstands electrical arcing. This prevents tracking and failure in high-voltage environments, enhancing the reliability and lifespan of electrical parts.

Reliable Mechanical & Thermal Strength

This grade maintains high mechanical strength and heat resistance (HDT up to 217°C). It ensures dimensional stability and performance under load and in high-temperature operating conditions.

glass filled VALOX FR PBT resin natural color

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top