Valox FR PBT 855 Flame Retardant Grade

VALOX™ FR resin 855 is a 15% glass-filled, flame-retardant PBT/PET compound. It offers a UL94 V-0 rating at 1.5mm, excellent chemical resistance, and superior aesthetics for demanding applications like appliances and lighting.

  • Character: 15% glass filled, flame retardant
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.
=

Key technical data

  • Flame Rating: UL 94 V-0 @ 1.5 mm
  • Heat Deflection Temp (HDT): 187°C @ 1.82 MPa
  • Tensile Strength (Break): 95 MPa
  • Flexural Modulus: 5000 MPa
  • Notched Izod Impact: 55 J/m
  • Relative Temperature Index (Elec): 125°C
  • Specific Gravity: 1.5
  • Mold Shrinkage (Flow): 0.4 – 0.6%

Application

  • Steam Irons (Base plates, housings)
  • Appliance Components (Motor housings, connectors, handles)
  • Lighting Parts (LED housings, reflectors, sockets)

Features & Benefits

Superior Flame Retardant Safety

VALOX 855 achieves a UL94 V-0 rating at just 1.5mm, ensuring critical fire safety in enclosed electrical devices and reducing risks in demanding applications.

Exceptional Heat & Dimensional Stability

With a Heat Deflection Temperature of 187°C at high stress, this resin maintains its shape and strength in high-heat environments like steam irons and oven components.

Excellent Processability & Aesthetics

VALOX™ FR resin 855 offers easy molding with high flow, leading to faster cycle times and superior surface quality for visible parts that also need to be durable.

15% glass filled VALOX FR PBT resin

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity
Scroll to Top