Valox FR PBT 865 Flame Retardant Grade
VALOX™ FR resin 865 is a 30% glass-filled, flame-retardant PBT/PET compound. It offers superior UL94 V-0 & 5VA ratings, excellent chemical resistance, and improved aesthetics, ideal for demanding electrical, appliance, and lighting components.
- Character: 30% glass filled, flame retardant
Key technical data
- Tensile Strength (Break): 130 MPa
- Flexural Modulus: 8,000 MPa
- Notched Izod Impact: 80 J/m
- HDT @1.82 MPa: 193 °C
- Relative Temp Index (Elec/Mech): 110 °C
- Flame Ratings UL 94 V-0: 1.5 mm
- Flame Ratings UL 94 5VA: 3.0 mm
- Specific Gravity: 1.66
- Mold Shrinkage (Flow): 0.3 – 0.5%
- Water Absorption (24hr): 0.03%
Download
Application
- Steam Irons & Garment Steamers: Bases and housings that resist high heat and steam.
- Appliance Components: Housings and structural parts for toasters, coffee makers, and power tools.
- Lighting Parts: Connectors, reflectors, and housings for both interior and exterior lighting systems.
- Electrical Components: Circuit breakers, switches, and connectors requiring flame retardancy.
Features & Benefits

Related Valox™ FR PBT Products
VALOX™ FR PBT V4860HR
VALOX™ FR PBT V4760
VALOX™ FR PBT V3900WX
VALOX™ FR PBT V3504
VALOX™ FR PBT SHF3800UX
VALOX™ FR PBT DR48
VALOX™ FR PBT 4631
VALOX™ FR PBT 4521
VALOX™ FR PBT 4512
VALOX™ FR PBT 3706
VALOX™ FR PBT 865
VALOX™ FR PBT 771
VALOX™ FR PBT 855
VALOX™ FR PBT 855
VALOX™ FR PBT 780
VALOX™ FR PBT 553U
VALOX™ FR PBT 457
VALOX™ FR PBT 420SE0
Advanced Manufacturing