VALOX™ FR PBT 3706

SABIC® PC Resin

Valox FR PBT 3706 Flame Retardant Grade

VALOX™ FR resin 3706 is an impact-modified, flame-retardant PBT/PC blend. It offers excellent chemical resistance and top-tier UL94 V-0 (1.5mm) & 5VA (2.49mm) ratings. It is suitable to outdoor electrical enclosures.

  • Character: unreinforced impact modified flame retardant, injection moldable grade
Drag & Drop Files, Choose Files to Upload You can upload up to 10 files.
* We prioritize your privacy and ensure information security.

Key technical data

  • Flame Ratings: UL 94 V-0 @ 1.5 mm / 5VA @ 2.49 mm
  • Tensile Strength at Yield: 48 MPa
  • Tensile Elongation at Break: 50%
  • Notched Izod Impact (23°C): 667 J/m
  • Heat Deflection Temp (1.82 MPa): 85 °C
  • Relative Temp Index (Electrical): 100 °C
  • Specific Gravity: 1.3
  • Melt Temperature (Processing): 250 – 265 °C

Application

  • Electrical and Utility Equipment
  • Telecommunications Housings
  • Industrial Control Boxes

Features & Benefits

Superior Flame Retardant Safety

This grade achieves UL94 V-0 at a thin 1.5mm, allowing for lighter, more compact part designs without compromising critical fire safety standards in electrical components.

Exceptional Impact & Toughness

With high notched Izod impact strength, VALOX 3706 withstands physical knocks, drops, and installation stresses, reducing breakage and ensuring product longevity in tough environments.

Reliable Performance Outdoors

It resists chemicals, moisture, and heat, maintaining its properties and structural integrity over time, which is perfect for outdoor enclosures exposed to the elements.

VALOX™ FR PBT resin natual color

Advanced Manufacturing

Extruder machine
High-speed mixer machine
Water ring pelletizer
Automatic bagging machine
Vibrating screening machine
Plastic rein material warehouse storage capacity