Valox FR PBT 4521 Flame Retardant Grade
VALOX™ FR resin 4521 is a 20% glass-filled, flame-retardant PBT. It offers high flow for easy molding, excellent chemical resistance, and top-tier safety ratings like UL94 V-0 at 0.75mm. It is suitable to thin-wall electrical components.
- Character: 20% glass filled, high flow, flame retardant
Key technical data
- Flame Ratings: UL 94 V-0 @ 0.75 mm | 5VA @ 2.0 mm
- Tensile Strength (Yield): 110 MPa
- Flexural Modulus: 6500 – 7000 MPa
- HDT @ 1.82 MPa: 205°C
- Vicat Softening Temp (B/50): 210°C
- Comparative Tracking Index (CTI): 275 V
- Dielectric Strength (0.8mm): 37 kV/mm
- Melt Temperature: 250 – 270°C
- Drying: 2-4 hours at 110-120°C
Download
Application
- Electrical Connectors & Sockets
- Circuit Breakers & Switches
- Automotive Sensors & Actuators
- Coil Formers & Bobbins
- Household Appliance Components
Features & Benefits

Related Valox™ FR PBT Products
VALOX™ FR PBT V4860HR
VALOX™ FR PBT V4760
VALOX™ FR PBT V3900WX
VALOX™ FR PBT V3504
VALOX™ FR PBT SHF3800UX
VALOX™ FR PBT DR48
VALOX™ FR PBT 4631
VALOX™ FR PBT 4521
VALOX™ FR PBT 4512
VALOX™ FR PBT 3706
VALOX™ FR PBT 865
VALOX™ FR PBT 771
VALOX™ FR PBT 855
VALOX™ FR PBT 855
VALOX™ FR PBT 780
VALOX™ FR PBT 553U
VALOX™ FR PBT 457
VALOX™ FR PBT 420SE0
Advanced Manufacturing