Valox FR PBT 4631 Flame Retardant Grade
VALOX™ FR Resin 4631 is a 30% glass-filled, flame-retardant PBT engineered for injection molding. It delivers superior mechanical strength, excellent electrical properties, and a critical UL94 V-0 flame rating for safe, reliable components.
- Character: 30% glass filled, flame retardant
Key technical data
- Tensile Strength (Yield): 130 MPa
- Flexural Strength: 200 MPa
- Flexural Modulus: 9000 – 9600 MPa
- Izod Impact, Notched (23°C): 80 J/m (ASTM)
- HDT @ 1.82 MPa: 205 °C
- Vicat Softening Temp (Rate B/50): 205 °C
- Relative Temp Index (Electrical): 130 °C
- Glow Wire Flammability Index (GWFI): 960 °C
- Flame Rating: UL 94 V-0 @ 0.75 mm
- Comparative Tracking Index (CTI): 250 V
- Volume Resistivity: >1.E+15 Ω·cm
- Filler Content: 30% Glass Fiber
- Specific Gravity: 1.67
- Mold Shrinkage (Flow): 0.1 – 0.3%
- Melt Temperature: 250 – 270 °C
- Drying Temperature: 110 – 120 °C
Download
Application
- Electrical Components: Circuit breakers, switches, and relay housings.
- Automotive Systems: Sensors, motor end caps, and under-hood connectors.
- Industrial Equipment: Power tool housings, control system housings, and coil bobbins.
- Consumer Appliances: Connectors and internal components in printers, smart meters, and power supplies.
Features & Benefits

Related Valox™ FR PBT Products
VALOX™ FR PBT V4860HR
VALOX™ FR PBT V4760
VALOX™ FR PBT V3900WX
VALOX™ FR PBT V3504
VALOX™ FR PBT SHF3800UX
VALOX™ FR PBT DR48
VALOX™ FR PBT 4631
VALOX™ FR PBT 4521
VALOX™ FR PBT 4512
VALOX™ FR PBT 3706
VALOX™ FR PBT 865
VALOX™ FR PBT 771
VALOX™ FR PBT 855
VALOX™ FR PBT 855
VALOX™ FR PBT 780
VALOX™ FR PBT 553U
VALOX™ FR PBT 457
VALOX™ FR PBT 420SE0
Advanced Manufacturing