Valox FR PBT SHF3800UX Flame Retardant Grade
VALOX™ FR Resin SHF3800UX is a flame-retardant PBT/PC blend offering superior impact strength, excellent flow for complex molds, and high thermal & chemical resistance. Ideal for demanding electrical components.
- Character: unreinforced, UV stabilized, impact modified flame retardant
Key technical data
- Flame Rating: UL 94 V-0 @ 0.75 mm / 5VA @ 2.5 mm
- Relative Temp Index (Electrical): 140 °C
- Tensile Strength at Yield: 50 MPa
- Izod Impact (Notched at 23°C): 40 kJ/m²
- Heat Deflection Temp (1.8 MPa): 85 °C
- Melt Temperature (Processing): 250 – 270 °C
- Density: 1.33 g/cm³
- CTE (Flow): 1.13 x 10⁻⁴ 1/°C
Application
- Bobbins and Coil Formers
- Circuit Breakers & Switches
- Electrical Enclosures & Housings
- Connectors and Sockets
- Other Critical Electrical Components
Features & Benefits

Related Valox™ FR PBT Products
VALOX™ FR PBT V4860HR
VALOX™ FR PBT V4760
VALOX™ FR PBT V3900WX
VALOX™ FR PBT V3504
VALOX™ FR PBT SHF3800UX
VALOX™ FR PBT DR48
VALOX™ FR PBT 4631
VALOX™ FR PBT 4521
VALOX™ FR PBT 4512
VALOX™ FR PBT 3706
VALOX™ FR PBT 865
VALOX™ FR PBT 771
VALOX™ FR PBT 855
VALOX™ FR PBT 855
VALOX™ FR PBT 780
VALOX™ FR PBT 553U
VALOX™ FR PBT 457
VALOX™ FR PBT 420SE0
Advanced Manufacturing