Valox FR PBT V4760 Flame Retardant Grade
VALOX™ FR resin V4760 is a 30% glass-filled, flame-retardant PBT offering high flow and excellent chemical resistance. It achieves top UL94V-0 flame rating at a thin 0.28mm, ideal for demanding electrical components.
- Character: 30% glass filled, high flow flame retardant, injection moldable grade with excellent chemical resistance.
Key technical data
- Flame Rating: UL 94 V-0 @ 0.28 mm, 5VA @ 1.5 mm
- Melt Volume Rate (MVR): 28 cm³/10min (250°C/5.0 kg)
- Heat Deflection Temp (HDT): 207°C @ 1.8 MPa
- Tensile Strength (Yield): 126 MPa (ISO 527)
- Flexural Modulus: 9500 MPa (ISO 178)
- Comparative Tracking Index (CTI): 250 V
- Density: 1.67 g/cm³
Download
Application
- Electrical Connectors
- Bobbins and Coil Formers
- Switches and Circuit Breakers
- Other Thin-Wall Electrical Components
Features & Benefits

Related Valox™ FR PBT Products
VALOX™ FR PBT V4860HR
VALOX™ FR PBT V4760
VALOX™ FR PBT V3900WX
VALOX™ FR PBT V3504
VALOX™ FR PBT SHF3800UX
VALOX™ FR PBT DR48
VALOX™ FR PBT 4631
VALOX™ FR PBT 4521
VALOX™ FR PBT 4512
VALOX™ FR PBT 3706
VALOX™ FR PBT 865
VALOX™ FR PBT 771
VALOX™ FR PBT 855
VALOX™ FR PBT 855
VALOX™ FR PBT 780
VALOX™ FR PBT 553U
VALOX™ FR PBT 457
VALOX™ FR PBT 420SE0
Advanced Manufacturing